ABSTRACT:
Copolymers are composed of
a) from 0.01 to 40% by weight of a copolymerized ethylenically unsaturated compound having at least one isocyanate group blocked with an oxime,
b) from 30 to 99.99% by weight of at least one C.sub.1 -C.sub.20 -alkyl (meth)acrylate, one vinyl ester of carboxylic acids of 1 to 20 carbon atoms, one vinylaromatic of up to 20 carbon atoms, one ethylenically unsaturated nitrile of 3 to 6 carbon atoms, one vinyl halide or one nonaromatic hydrocarbon of 4 to 8 carbon atoms having at least 2 conjugated double bonds,
c) from 0 to 30% by weight of at least one comonomer having at least one keto or aldehyde group and
d) from 0 to 50% by weight of at least one further monomer.
REFERENCES:
patent: 5268417 (1993-12-01), Filges et al.
Bauer Gerhard
Haeberle Karl
Maempel Lothar
BASF - Aktiengesellschaft
Sarofim N.
Schofer Joseph L.
LandOfFree
Copolymers crosslinking at room temperature does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Copolymers crosslinking at room temperature, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Copolymers crosslinking at room temperature will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1406431