Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – From sulfur-containing reactant
Patent
1981-09-01
1983-02-01
Marquis, Melvyn I.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
From sulfur-containing reactant
C08G 7514
Patent
active
043716717
ABSTRACT:
A method for dehydrating pre-polymerization mixtures in the preparation of poly(arylene sulfide) in which a reaction mixture of a sulfur source and an organic amide are contacted at an essentially constant pressure within a range of about 4 psig to about 40 psig and a first temperature in a range of about 300.degree. F. to 400.degree. F. to form a complex of the reactants with the mixture subsequently maintained at essentially constant pressure while elevating the temperature to a second temperature at which, at the chosen pressure, essentially all water is removed from the mixture. Other compounds including bases, alkali metal carboxylates, alkali metal carbonates, lithium halides, and lithium borate can be present in the reaction mixture. Preferably the sulfur source is sodium sulfide and the organic amide is N-methylpyrrolidone.
REFERENCES:
patent: 3354129 (1967-11-01), Edmonds, Jr. et al.
patent: 3867356 (1975-02-01), Campbell
patent: 3919177 (1975-11-01), Campbell
patent: 4025496 (1977-05-01), Anderson et al.
patent: 4038259 (1977-07-01), Campbell et al.
patent: 4038262 (1977-07-01), Edmonds, Jr.
patent: 4038263 (1977-07-01), Edmonds, Jr. et al.
patent: 4039518 (1977-08-01), Campbell
patent: 4056515 (1977-11-01), Vidaurri, Jr.
patent: 4064114 (1977-12-01), Edmonds, Jr.
Marquis Melvyn I.
Phillips Petroleum Company
LandOfFree
Controlled, elevated pressure dehydration of poly(arylene sulfid does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Controlled, elevated pressure dehydration of poly(arylene sulfid, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Controlled, elevated pressure dehydration of poly(arylene sulfid will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2408058