ABSTRACT:
A continuous hot dip aluminum coating method used in a continuous hot dip aluminum coating line for hot dip aluminum coating on steel in Sendzimir method or nonoxidizing furnace method, said method comprising the covering the surface of the coating bath in the snout of said hot dip coating line by use of an inert gas atmosphere.
REFERENCES:
patent: 4053663 (1977-10-01), Caldwell
patent: 4441936 (1984-03-01), Takahashi
patent: 4466999 (1984-08-01), Leonard
patent: 4478892 (1984-10-01), Amberson
Asakawa Kenichi
Higuchi Seizun
Okada Nobuyoshi
Nippon Steel Corporation
Silverberg Sam
LandOfFree
Continuous hot dip aluminum coating method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Continuous hot dip aluminum coating method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Continuous hot dip aluminum coating method will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1914949