ABSTRACT:
A continuous casting chill mold, for the continuous casting of metals, particularly of steel, comprises a water-cooled interior section and an outer jacket section which avoids the problems associated with the machining of the cooling channels and at the same time reduces wastage, in that the interior section is produced by chipless (i.e. non-machining) production methods as a thin-walled sleeve having a dense microstructure, the interior section is surrounded by a coiled cooling pipe which, together with the interior section, is positively materially bonded to the outer jacket section consisting of copper applied by casting techniques. Neither in the cooling zone nor in the wall region of the mold cavity is there any risk of cutting into pores or pipes because all chip-removing machining is dispensed with.
REFERENCES:
patent: 34472 (1962-02-01), Babbitt
patent: 3853309 (1974-12-01), Widmer
patent: 4197902 (1980-04-01), Von Jan et al.
patent: 4276994 (1981-07-01), Spalding
LandOfFree
Continuous casting mould does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Continuous casting mould, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Continuous casting mould will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-606626