Metal deforming – With use of control means energized in response to activator... – Metal deforming by use of roller or roller-like tool element
Patent
1994-08-22
1997-03-11
Bray, W. Donald
Metal deforming
With use of control means energized in response to activator...
Metal deforming by use of roller or roller-like tool element
72 118, 72234, 723652, B21B 3702
Patent
active
056090536
ABSTRACT:
This invention relates to a method and apparatus for improving rolling mill efficiency by providing modified fixed setup parameters according to the class of the material being rolled through the following steps: (1) divide the products produced by the rolling mill into hardness/rollability classes; (2) empirically establish a set of fixed interstand thicknesses for each class which produce desired operational characteristics, such as constant thermal operation; and (3) vary the entry thickness for a particular product in accordance with the set of fixed interstand thicknesses for its class proportionally based on the desired exit thickness.
REFERENCES:
patent: 3820366 (1974-06-01), Smith, Jr.
patent: 5054302 (1991-10-01), Yamashita et al.
Ferreira Adriano M. P.
Horton Terry L.
Alcan Aluminum Corporation
Bray W. Donald
Schoeffler Thomas C.
LandOfFree
Constant reduction multi-stand hot rolling mill set-up method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Constant reduction multi-stand hot rolling mill set-up method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Constant reduction multi-stand hot rolling mill set-up method will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-436104