ABSTRACT:
For making a ductile boron-containing grain-oriented silicon steel, there is practiced, at a late stage in the making of the product either during the final texture anneal or a subsequent anneal, a high-temperature anneal in a reducing atmosphere with the use of a separating-agent coating, particularly magnesium oxide, which contains an effective amount of a compound of molybdenum and/or tungsten.

REFERENCES:
patent: 3151000 (1964-09-01), Schmidt et al.
patent: 3785879 (1974-01-01), Lee et al.
patent: 3941621 (1976-03-01), Lee et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Composition for deboronizing grain-oriented silicon steel does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Composition for deboronizing grain-oriented silicon steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Composition for deboronizing grain-oriented silicon steel will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-638532

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.