Chemistry: electrical current producing apparatus – product – and – With pressure equalizing means for liquid immersion operation
Reexamination Certificate
2004-05-22
2009-06-23
Mulcahy, Peter D. (Department: 1796)
Chemistry: electrical current producing apparatus, product, and
With pressure equalizing means for liquid immersion operation
C429S006000, C429S188000, C429S199000, C429S314000, C524S602000
Reexamination Certificate
active
07550216
ABSTRACT:
The present invention relates to composite solid polymer electrolyte membranes (SPEMs) which include a porous polymer substrate interpenetrated with a water soluble ion-conducting material. SPEMs of the present invention are useful in electrochemical applications, including fuel cells and electrodialysis.
REFERENCES:
patent: 3284238 (1966-11-01), White
patent: 3528954 (1970-09-01), Carlson
patent: 4110265 (1978-08-01), Hodgdon
patent: 4116888 (1978-09-01), Ukihashi et al.
patent: 4138373 (1979-02-01), Ukihashi et al.
patent: 4138426 (1979-02-01), England
patent: 4191811 (1980-03-01), Hodgdon
patent: 4273903 (1981-06-01), Rose
patent: 4330654 (1982-05-01), Ezzell et al.
patent: 4358412 (1982-11-01), Ezzell et al.
patent: 4413106 (1983-11-01), Coplan et al.
patent: 4714663 (1987-12-01), Arnold, Jr. et al.
patent: 4814399 (1989-03-01), Sansone et al.
patent: 4845150 (1989-07-01), Kovak et al.
patent: 4865930 (1989-09-01), Kindler et al.
patent: 5013765 (1991-05-01), Sluma et al.
patent: 5080698 (1992-01-01), Krizan
patent: 5168011 (1992-12-01), Kovar et al.
patent: 5202165 (1993-04-01), Lusignea et al.
patent: 5259950 (1993-11-01), Shiro et al.
patent: 5271813 (1993-12-01), Linkous
patent: 5288529 (1994-02-01), Harvey et al.
patent: 5300206 (1994-04-01), Allen et al.
patent: 5348569 (1994-09-01), Bikson et al.
patent: 5362836 (1994-11-01), Helmer-Metzmann et al.
patent: 5403675 (1995-04-01), Ogata et al.
patent: 5422411 (1995-06-01), Wei et al.
patent: 5438082 (1995-08-01), Helmer-Metzmann et al.
patent: 5501831 (1996-03-01), Kovar et al.
patent: 5525436 (1996-06-01), Savinell et al.
patent: 5547551 (1996-08-01), Bahar et al.
patent: 5561202 (1996-10-01), Helmer-Metzmann et al.
patent: 5585039 (1996-12-01), Matsumoto et al.
patent: 5599614 (1997-02-01), Bahar et al.
patent: 5599638 (1997-02-01), Surampudi et al.
patent: 5599639 (1997-02-01), Sansone et al.
patent: 5609795 (1997-03-01), Matsumoto et al.
patent: 5635041 (1997-06-01), Bahar et al.
patent: 5656389 (1997-08-01), Tetzlaff et al.
patent: 5723086 (1998-03-01), Ledjeff et al.
patent: 5773162 (1998-06-01), Surampudi et al.
patent: 6524665 (2003-02-01), Sahouani et al.
patent: 2004/0028973 (2004-02-01), Pan et al.
patent: 42 43 600 (1993-07-01), None
patent: 0 008 895 (1980-03-01), None
patent: 008895 (1980-03-01), None
patent: 0 227 299 (1987-07-01), None
patent: 0 277 834 (1988-08-01), None
patent: 4204522 (1992-07-01), None
patent: 5326037 (1993-12-01), None
patent: 6029032 (1994-02-01), None
patent: 6242474 (1994-09-01), None
patent: WO-96/13872 (1996-05-01), None
patent: WO-96/18216 (1996-06-01), None
patent: WO-96/29360 (1996-09-01), None
patent: WO-96/40798 (1996-12-01), None
patent: WO-97/24777 (1997-10-01), None
patent: WO-96/05707 (1997-11-01), None
patent: WO-98/11614 (1998-03-01), None
patent: WO-98/22989 (1998-05-01), None
U.S. Appl. No. 09/262,861, Formato et al.
U.S. Appl. No. 09/261,349, Formato et al.
Database WPI, sec. Ch., Week 198049, Derwent Publications, Ltd., London, GB; Class A25, AN 1980-87481C, XP002164079. JP 55137005 A, Teijin Ltd., Oct. 25, 1980.
Database WPI, sec. Ch., Week 198434, Derwent Publications, Ltd., London, GB; Class A88, AN 1984-209372, XP002164080. JP 59120211 A, Asahi Glass Co. Ltd., Jul. 11, 1984.
A.B. LaConti, et al., “Solid Polymer Electrolyte Electrochemical Cells: Electrode and Other Materials Considerations”, General Electric Company, Wilmington, MA 1974, pp. 354-374.
Ueda, et al., “Synthesis and Characterization of Aromatic PES Containing Pendant Sodium Sulfonate Groups”, J. Polymer Science, vol. 31, 1993, p. 853-858.
Kerres, et al., “New Ionomers and Their Applications in PEM Fuel Cells”, ICE, Stuttgart, Germany, 1998, pp. 1951-1956.
Kreuer, K. D., “Membrane Materials for PEM Fuel Cells: A Microstructural Approach”, Electrochemical Society Proceedings, vol. 95-23, pp. 241-246.
Xu, et al., “Preliminary Study of Phosphonate Ion Exchange Membranes for PEM Fuel Cells”, SUNY, Syracuse, NY, 1996, 2 pgs.
Kolde, et al., “Advanced Composite Polymer Electrolyte Fuel Cell Membranes”, Electrochemical Society Proceedings, vol. 95-23, pp. 193-201.
Ren, et al., “Methanol Cross-over in Direct Methanol Fuel Cells”, Electrochemical Society Proceedings, vol. 95-23, 1995, pp. 284-298.
Jones, D.J., et al., “New Proteon Conductors For Fuel Cell Applications”, Enviornmental Research Forum, vols. 1-2 (1996), p. 115-126.
F. KuCera, et al., “Homogeneous and Heterogeneous Sulfonation of Polymers: A Review”, Polymer Engineering and Science, May 1998, vol. 36, No. 5, pp. 783-792.
Tsuchida, et al., “Synthesis and Proton Conductivity of Highly Sulfonated Poly (thiophenylene)”, Macromolecules, 1997, vol. 30, pp. 2941-2946.
M. Kurihara, et al., “The Major Developments of the Evolving Reverse Osmosis Membranes and Ultrafiltration Membranes”, Polymer Journal, vol. 23, No. 5, pp. 513-520.
P. Clemenson, et al., “Synthesis and Characterization of New Water-Soluable Precursors of Polyimides”, Polymer Engineering and Science, Jun. 1997, vol. 37, No. 6, pp. 966-977.
L.H. Sperling, et al, “The Current Status of Interpreting Polymer Networks”, IPNs Around the World, Edited by S.C. Kim and L.H. Sperling, 1997 John Wiley & Sons, Ltd.
A.B. LaConti, et al., “Morphology And Reverse Osmosis Properties of Sulfonated 2,6-Dimethyl Polyphenylene Oxide Membranes”, Reprinted from Reverse Osmosis Membrane Research, 1972, pp. 263-284.
D. Weng, et al., “Electo-osmotic Drag Coefficient of Water and Methanol in Polymer Electrolytes at Elevated Temperatures”, J. Electrochem. Soc., vol. 143, No. 4, Apr. 1996, pp. 1260-1263.
A.V. Anantaraman, et al., “Studies on Ion-exchange Membranes. Part 1 Effect of Humidity on the Conductivity of Nafion”, Journal of Electroanalytical Chemistry, 414 (1996), pp. 115-120.
Y. Sone, et al, “Proton Conductivity of Nafion 117 as Measured by a Four-Electrode AC Impedance Method”, J. Electrochem. Soc., vol. 143, No. 4, Apr. 1996, pp. 1254-1259.
M. Schulze, et al., “Proton Exchange With Alkaline Ions in Nafion”, six pages.
J.J. Sumner, et al., “Proton Conductivity in Nafion 117 and in a Novel Bis [(perfluoroalkyl)sulfonyl]imide Ionomer Membrane”, J. Electrochem. Soc., vol. 145, No. 1, Jan. 1998, pp. 107-111.
T. Okada, et al., “Transport And Equilibrium Properties of Nafion Membranes With H+ and Na+Ions”, Journal of Electroanalytical Chemistry, 442 (1998), pp. 137-145.
J. Kerres, et al., “Development and Characterization of Crosslinked Ionomer Membranes Based Upon Sulfinatedand Sulfonated PSU Crosslinked PSU Blend Membranes By Disproportionation of Sulfinic Acid Groups”, Journal of Membrane Science, 239 (1998) pp. 211-225.
N.M. Belomonia, et al., “Thermoreactive Sulfur-Containing Poly(phenylquinoxaline)s”, Polymer Science, Series B, vol. 38, Nos. 1-2, 1996, pp. 98-100.
T. Kobayashi, et al., “Proton-Conducting Polymers Derived from Poly(ether-etherketone) and Poly(4-phenoxybenzoyl-1-1,4-phenylene)”, Solid State Ionics, 106 (1998), pp. 219-225.
G. Alberti, et al., “Layered metal IV Phos phonates, a Large Class of inorgano-organic Proton Conductors”, Solid State Ionics, 97, (1997), p. 177-186.
Y. Uchimoto, et al., “Ionically Conductive Thin Polymer Films Prepared by Plasma Polymerization, Part 7. Preparation and Characterization of Solid Polymer Electrolyte Having Fixed Carboxylic Acid Groups with Single Mobile Species”, Solid State Ionics, 40/41 (1990), pp. 624-627.
T.A. Zawadzinski, Jr., et al., “Water Uptake by and Transport Through Nafion 117 Membranes”, Journal of the Electrochemical Society, vol. 40, No. 4, Apr. 1993, pp. 1041-1047.
R.W., Kopitzke, et al, “Sulfonation of Poly(phenylquinoxaline) Film”, Journal of Polymer Science: Part A: Polymer Chemistry, vol. 86 (1998), pp. 1197-1199.
PCT International Search Report (Form PCT/IS
Kovar Robert F.
Nair Bindu R.
Ofer David
Stoler Emily J.
Conlin David G.
Edwards Angell Palmer & & Dodge LLP
Foster-Miller Inc.
Hu Henry
Mulcahy Peter D.
LandOfFree
Composite solid polymer electrolyte membranes does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Composite solid polymer electrolyte membranes, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Composite solid polymer electrolyte membranes will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4079580