ABSTRACT:
An article exhibiting superior mechical properties and resistance to oxidation corrosion at elevated temperatures as described. The article has particular utility in gas turbine engines and is comprised of a nickel base superalloy consisting essentially of 3-10% Cr, 12.1-16% Co, 1.0-1.9% Mo, 3-10% W, 0-5% Re, 4-7% Al, 0-1.5% Ti, 0-8% Ta, 0.5-3% Hf, 0-2% Cb, 0-1% V, 0.02-0.12% Zr, 0.03-0.2% C, 0.005-0.25% B, 0-0.15% of an oxygen active element such as yttrium, balance essentially nickel. This composition is melted and directionally solidified in columnar grain form to provide useful articles.

REFERENCES:
patent: 3293030 (1966-12-01), Child et al.
patent: 3526499 (1970-09-01), Quigg et al.
patent: 3681061 (1972-08-01), Fletcher
patent: 3711337 (1973-01-01), Sullivan et al.
patent: 3765879 (1973-10-01), Hockin et al.
patent: 4006012 (1977-02-01), Kadlimann
patent: 4043841 (1977-08-01), Bibring et al.
patent: 4083734 (1978-04-01), Boesch
patent: 4093454 (1978-06-01), Saito et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4279645 (1981-07-01), Brown
patent: 4374084 (1983-02-01), Meethan et al.
patent: 4388124 (1983-06-01), Henry

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Columnar grain superalloy articles does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Columnar grain superalloy articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Columnar grain superalloy articles will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2385365

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.