Alloys or metallic compositions – Containing over 50 per cent metal but no base metal – Iron containing
Patent
1981-03-05
1983-11-15
Dean, R.
Alloys or metallic compositions
Containing over 50 per cent metal but no base metal
Iron containing
148442, 420582, 420586, C22C 3000
Patent
active
044155328
ABSTRACT:
Disclosed is a cobalt-base superalloy containing about 32% cobalt, 8% nickel, 26.5% chromium, 2.5% tungsten, 5% niobium, about 1% each manganese and silicon, about 0.4% carbon, and the balance about 23% iron plus incidental impurities and modifiers normally found in alloys of this class. The alloy is readily processed in the form of wrought products, castings, metal powder and all forms of welding and hardfacing materials. The outstanding characteristics of the new alloy include the resistance to cavitation erosion and galling, low cost and minimal use of strategic metals.
REFERENCES:
patent: 2974037 (1961-03-01), Thielemann
Cabot Corporation
Dean R.
Phillips Joseph J.
Schuman Jack
LandOfFree
Cobalt superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Cobalt superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Cobalt superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-159185