ABSTRACT:
A nickel-zinc galvanic cell is provided, having a zinc oxide negative electrode, a nickel oxide positive electrode, and an alkaline electrolyte. Chemical additives are placed in each of the negative and positive electrodes. The positive nickel hydroxide electrode contains a mixture of cobalt oxide contained within a nickel oxide matrix in the range of about 1% to 10%, and cobalt metal in the range of about 1% to 10%, by weight. The negative zinc oxide electrode may contain oxides other than the oxide of zinc, which have redox potentials which are negative of −0.73 volts. Also, the metal oxide additives to the negative zinc oxide electrode are such as to inhibit release of soluble cobalt from the nickel oxide negative electrode prior to a formation charge being applied to the electrochemical cell.
REFERENCES:
patent: 3647544 (1972-03-01), Schneider
patent: 3870564 (1975-03-01), Takamura et al.
patent: 3951687 (1976-04-01), Takamura et al.
patent: 3961985 (1976-06-01), Takamura et al.
patent: 4003754 (1977-01-01), Winsel et al.
patent: 4017665 (1977-04-01), Sandera et al.
patent: 5215836 (1993-06-01), Eisenberg
patent: 5523182 (1996-06-01), Ovshinsky et al.
patent: 5804334 (1998-09-01), Yamamura et al.
patent: 5968684 (1999-10-01), Hayashi et al.
patent: 6040007 (2000-03-01), Junichi et al.
patent: 6225004 (2001-05-01), Hayashi
patent: 6436575 (2002-08-01), Weckesser et al.
patent: 6617072 (2003-09-01), Venkatesan et al.
patent: 6649305 (2003-11-01), Bugnet et al.
patent: 6787265 (2004-09-01), Phillips
patent: 7261972 (2007-08-01), Inada et al.
patent: 2002/0037455 (2002-03-01), Tani et al.
patent: 2002/0172758 (2002-11-01), Tetsuo
patent: 2003/0140483 (2003-07-01), Wakabayashi et al.
patent: 2004/0115533 (2004-06-01), Phillips
patent: 2006/0029863 (2006-02-01), Miyamoto et al.
patent: 2009/0202904 (2009-08-01), Geng et al.
patent: 2009/0208839 (2009-08-01), Geng et al.
patent: 0833397 (1976-04-01), None
patent: 0457354 (1991-11-01), None
patent: 0697746 (1996-02-01), None
patent: 0 902 490 (1999-03-01), None
patent: 1 172 869 (2002-01-01), None
patent: 1207576 (2002-05-01), None
patent: 1207576 (2002-05-01), None
patent: 1 367 666 (2003-12-01), None
patent: 1 699 099 (2006-09-01), None
patent: 54163324 (1979-12-01), None
patent: 56-29345 (1981-07-01), None
patent: 07037609 (1995-02-01), None
patent: 11297352 (1999-10-01), None
patent: 20058062 (2000-02-01), None
patent: 2005 056 733 (2005-03-01), None
“WordNet Search.” WordNet. Apr. 4, 2008 <http://wordnet.princeton.edu>.
“WordNet Search.” WordNet. Dec. 3, 2008. <http://wordnet.princeton.edu/perl/webwn?s=embedded>.
“WordNet Search.” WordNet. Dec. 3, 2008. <http://wordnet.princeton.edu/perl/webwn?s=paste>.
Ohta et al., “Nicel Hydroxide Electrode: Improvement of Charge Efficiency at High Temperature,” The Electrochemical Society Proceedings, vol. 94-27, pp. 296-302, 1994.
Canada Office Action dated Apr. 30, 2008, from corresponding Canadian Patent Application No. 2,325,640.
International Search Report mailed Apr. 29, 2002, PCT Application PCT/UCA01/01717.
Japan Office Action dated Feb. 22, 2008, from corresponding Japan Patent Application No. 2002-541747, with English explanation from Japanese Associate of Office Action.
Japan Abstract, dated Feb. 25, 2000, from Japan Patent Application No. 2002-541747.
Search Report and Written Opinion dated May 13, 2009 for corresponding PCT Application No. PCT/US2009/033265.
Ying et al., “Surface modification of nickel hydroxide particles by micro-sized cobalt oxide hydroxide and properties as electrode materials,”Surface and Coatings Technology, Elsevier, Amsterdam, NL, vol. 200, No. 7, (Dec. 21, 2005), pp. 2376-2379, XP005181204.
Canada Office Action dated Apr. 14, 2009, from Canadian Patent Application No. 2,325,640.
Japan Office Action dated Sep. 8, 2009, from Japan Patent Application No. 2002-541747, with English explanation from Japanese Associate of Office Action.
European Office Action dated Dec. 2, 2009 issued in 01993957.8.
PCT International Search Report and Written Opinion dated Jun. 22, 2010, from PCT Application No. PCT/US2010/033023.
Best Zachary
PowerGenix Systems, Inc.
Weaver Austin Villeneuve & Sampson LLP
Yuan Dah-Wei D
LandOfFree
Cobalt containing positive electrode formulation for a... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Cobalt containing positive electrode formulation for a..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Cobalt containing positive electrode formulation for a... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4197457