ABSTRACT:
An apparatus for coating a glass ribbon has an exhaust on each side of a coating unit at different distances therefrom. With this arrangement, portions of the ribbon upstream and downstream of the coating unit are exposed to coating vapors from the coating unit for different periods of time. A coating mixture includes tin containing precursors and a silicon containing precursor. The silicon containing precursor has the structural formula ##STR1## where R.sub.1 is a group which does not have an oxygen available to form a peroxide, R.sub.2 is a functional group giving the silicon containing precursor the ability to be easily converted to silicon oxide coating, R.sub.3 is a bridging group to provide for multiple silicon atoms and R.sub.4 completes the bonding on the foundation silicon atom. An accelerant e.g. a phosphorus containing precursor may be used with the metal containing precursors to increase the deposition rate of the coating. The coating deposited on the glass has regions of continuously varying weight percent of silicon oxide and tin oxide as the distance from the glass-coating interface increases, with the surface of the coating farthest from the glass-coating interface being predominantly tin oxide. The regions within the coating provide the coating with different indices of refraction to eliminate iridescence resulting from increased thickness of the tin oxide at the outer coating surface and to provide the coated glass article with a neutral color. When phosphorus is used as the accelerant, the percent of crystallinity is reduced and approaches O, thereby reducing or eliminating the coating haze.

REFERENCES:
patent: 3378396 (1968-04-01), Zaromb
patent: 3674453 (1972-07-01), Loukes et al.
patent: 3681042 (1972-08-01), Edwards et al.
patent: 4146657 (1979-03-01), Gordon
patent: 4187336 (1980-02-01), Gordon
patent: 4206252 (1980-06-01), Gordon
patent: 4265974 (1981-05-01), Gordon
patent: 4308316 (1981-12-01), Gordon
patent: 4377613 (1983-03-01), Gordon
patent: 4386117 (1983-05-01), Gordon
patent: 4419386 (1983-12-01), Gordon
patent: 4440822 (1984-04-01), Gordon
patent: 4468420 (1984-08-01), Kawahara et al.
patent: 4469045 (1984-09-01), Chesworth
patent: 4590096 (1986-05-01), Lindner
patent: 4853257 (1989-08-01), Henery
patent: 4894352 (1990-01-01), Lane et al.
patent: 5168003 (1992-12-01), Proscia
patent: 5221352 (1993-06-01), Terneu et al.
Strong, J.; "Practical Application of High and Low-Reflecting Films on Glass", Le Journal De Physiques Et Le Radium, Jul. 11, 1950; pp. 441-443.
Delperier, B. et al.; "Analysis and Modelling of Tetraethoxysilane Pyrolysis"; Journal of Analytical and Applied Pyrolysis, 13, (1988), pp. 141-149.
Inoue, K. et al.; "Low Temperature Growth of SiO.sub.2 Thin Film by Double-Excitation Photo-CVD"; Japanese Journal of Applied Physics; vol. 26, No. 6, Jun. 1987, pp. 805-811.
Toyoda, Y. et al.; "Preparation of SiO.sub.2 Film by Photo-Induced Chemical Vapor Deposition Using a Deuterium Lamp and Its Annealing Effect"; Japanese Journal of Applied Physics; vol. 26, No. 6, Jun. 1987, pp. 835-840.
Chang, C. P. et al.; "Ion and Chemical Radical Effects on the Step Coverage of Plasma Enchanced Chemical Vapor Deposition Tetraethylorthosilicate Films"; J. Appl. Phys.; 67(4), 15 Feb. 1990.
Niwano, M. et al.; "Low-Temperature Deposition of Silicon Dioxide Films by Photoinduced Decomposition of Tetraethyoxysilane"; Japanese Journal of Applied Physics; vol. 28, No. 7, Jul. 1989, pp. L1310-L1313.
Taylor, R. C. et al.; "Hexachlorodisilane as a Precursor in the LPCVD of Silicon Dioxide and Silicon Oxynitride Films"; J. Electrochem. Soc.; vol. 136, No. 8, Aug. 1989, pp. 2382-2386.
Okuhara, T. et al.; "Preparation of SiO.sub.2 Overlayers on Oxide Substrates by Chemical Vapor Deposition of Si(OC.sub.2 H.sub.5).sub.4 "; Applied Surface Science, 29, (1987), pp. 223-241.
Chapple-Sokol, J. D. et al.; "A Kinetics Study of the Atomspheric Pressure CVD Reaction of Silane and Nitrous Oxide"; J. Electrochem. Soc., vol. 136, No. 10, Oct. 1989, pp. 2993-3003.
Hochberg, A. K. et al.; "The Use of Liquid Sources in CVD Applications: Fire Safety Considerations and Delivery Methods"; Technical Article 15 of J. C. Schumacker, a Unit of Air Products and Chemicals, Inc.
Crowell, J. E. et al.; "Model Studies of Dielectric Thin Film Growth: Chemical Vapor Deposition of SiO.sub.2 "; pp. 1864-1870.
Pavelescu, C. et al.; "Correlations Between the Properties and the Deposition Kinetics of Low-Temperature Chemical Vapour Deposited SiO.sub.2 Films: The Effect of O.sub.2 /SiH.sub.4 Mole Ratio"; Journal of Materials Science Letters, 9, (1990), pp. 143-144.
Lucovsky, G. et al.; "Deposition of Silicon Oxide, Nitride and Oxynitride Thin Films by Remote Plasma Enhanced Chemical Vapor Deposition"; Journal of Non-Crystalline Solids; 90, (1987), pp. 259-266.
Orfescu, C. et al.; "An Etch Rate Study on Thermally Annealed SiO.sub.2 Films Deposited in a TESO-LPCVD System"; Journal of Materials Science, 25, (1990), pp. 1366-1368.
Maruyama, Toshiro et al.; "Silicon Dioxide Thin Films Prepared by Chemical Vapor Deposition from Silicon Tetraacetate"; Japanese Journal of Applied Physics; vol. 28, No. 12, Dec. 1989, pp. L2253-L2254.
Ozturk, Mehmet C. et al.; "Low-Pressure Chemical Vapor Deposition of Polycrystalline Silicon and Silicon Dioxide by Rapid Thermal Processing", Mat. Res. Soc. Symp. Proc., vol. 146, (1989), pp. 109-114.
Webb, Douglas A. et al.; "Silicon Dioxide Films Produced by PECVD of TEOS and TMCTS"; Proc. 2nd International ULSI Science and Technology Symposium, ECS Proc., vol. 89(9), (1989), pp. 571-578.
Hochberg, A. K. et al.; "The LPCVD of Silicon Oxide Films below 400.degree. C. from Liquid Sources", J. Electrochem. Soc., vol. 136, No. 6, Jun. 1989, pp. 1843-1844.
Hochberg, Dr. A. et al.; "User's Guide For: Glass Deposition with LTO-410.TM. Source Material".
Desu, S. B., "Decomposition Chemistry of Tetraethoxysilane"; Abstract No. 1855RNP; presented at the Fall Meeting of Electrochemical Society, Honolulu, Hi., 18-23 Oct., 1987.
Raju, Surya K. et al.; "Analytical Model for the Low Pressure Chemical Vapor Deposition of SiO.sub.2 from Tetraethoxysilane".
J. C. Schumacher Co., Tetramethylcyclotetrasiloxane "Tomcats.TM."; Chemical & Physical Properties.
Hochbach, A. K. et al.; "The Deposition of Silicon Oxide Films at Low Temperatures from Liquid Sources".
Roy A. Gordon; Patent and Patent Citations.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Coating apparatus, method of coating glass, compounds and compos does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Coating apparatus, method of coating glass, compounds and compos, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Coating apparatus, method of coating glass, compounds and compos will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2371178

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.