ABSTRACT:
A component made of superalloy is provided with a localized coating formed from three layers by a brazing heat treatment, the layers comprising an outer layer having a composition adapted to the specific surface properties sought, an inner layer having a composition which includes flux elements, and an intermediate layer obtained by the deposition of a mixture of the materials used for the other two layers.
REFERENCES:
patent: 2431660 (1947-11-01), Gaudenzi
patent: 3719519 (1973-03-01), Perugini
patent: 3849865 (1974-11-01), Gedwell
patent: 3975165 (1976-08-01), Elbert et al.
patent: 4123594 (1978-10-01), Cheng
patent: 4481237 (1984-11-01), Bosshart et al.
patent: 4612256 (1986-09-01), Neuhauser et al.
patent: 4705203 (1987-11-01), McComas et al.
patent: 4778649 (1988-10-01), Niino et al.
patent: 5021629 (1991-06-01), Shinomura
patent: 5236116 (1993-08-01), Solanki et al.
Societe Nationale d'Etude et de Construction de Motors d'Aviatio
Zimmerman John
LandOfFree
Coated superalloy component does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Coated superalloy component, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Coated superalloy component will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-991151