ABSTRACT:
A protective coating is provided on gas turbine engine type superalloys comprising an interlayer adjacent the superalloy substrate a principal protective element of which comprises an aluminide of the basis metal of the substrate formed by the reaction of aluminum at high temperature with the substrate, and an overlayer comprising an MCrAlY-type coating where M is selected from the group consisting of cobalt, nickel and iron.
REFERENCES:
patent: 3542530 (1970-11-01), Talboom et al.
patent: 3649225 (1972-03-01), Simmons
patent: 3676085 (1972-07-01), Evans et al.
patent: 3754903 (1973-08-01), Goward et al.
patent: 3869779 (1975-03-01), Gedwill et al.
James Richard N.
Rutledge L. Dewayne
United Technologies Corporation
Weise E. L.
LandOfFree
Coated superalloy article does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Coated superalloy article, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Coated superalloy article will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1089632