Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...
Patent
1988-05-13
1989-11-21
Securro, Carman J.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Mixing of two or more solid polymers; mixing of solid...
525211, 525237, 525345, 524490, 524232, C08L 700, C08L 2316, C08L 2320, C08L 700
Patent
active
048823872
ABSTRACT:
NR/EPDM co-cured rubber blends with sulfur and organic peroxide used together as the co-curing agents to achieve ozone resistant, high tensile property rubber compositions. Sulfur accelerators MBTS and DPG are also employed in the curing process. NR/EPDM blends of from 70/30 to 55/45 are cured in an air cure process with sulfur in the range of 0.64-1.6 phr and with organic peroxide in the range of 0.6-1.6 phr.
REFERENCES:
patent: 2909584 (1959-10-01), Parks
patent: 3419639 (1968-12-01), Gentile
patent: 3658732 (1972-04-01), Ballini et al.
patent: 3817952 (1974-06-01), Knabeschuk
patent: 3821134 (1974-06-01), Son et al.
patent: 3830881 (1974-08-01), Woods et al.
patent: 4051083 (1977-09-01), Newman
"Peroxide Cross-linking: . . . " van Drumpt Rubber World 3/88 pp. 33-41.
"Co-vulcanization in NR/EPDM Blends" Tobing Rubber World-2/88-pp. 33-37.
Lamb Charles G.
Securro Carman J.
LandOfFree
Co-curing of NR/EPDM rubber bands does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Co-curing of NR/EPDM rubber bands, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Co-curing of NR/EPDM rubber bands will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1426641