ABSTRACT:
A nickel base superalloy composition consisting essentially of, in weight %, 9.3-10.0% Co, 6.4-6.8% Cr, 0.5-0.7% Mo, 6.2-6.6% W, 6.3-6.7% Ta, 5.45-5.75% Al, 0.8-1.2% Ti, 0.07-0.12% Hf, 2.8-3.2% Re, and balance essentially Ni wherein a carbon concentration of about 0.01 to about 0.08 weight % is provided for improving the cleanliness of a single crystal investment casting produced therefrom.
REFERENCES:
patent: 3567526 (1971-03-01), Gell et al.
patent: 3620852 (1971-11-01), Herchenroeder et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4402772 (1983-09-01), Duhl et al.
patent: 4643782 (1987-02-01), Harris et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 4801513 (1989-01-01), Duhl et al.
patent: 5100484 (1992-03-01), Wukusick et al.
Baker Robert J.
Corrigan John
Leonard Eric L.
Mihalisin John R.
Vandersluis Jay L.
Howmet Research Corporation
Timmer Edward J.
Yee Deborah
LandOfFree
Clean single crystal nickel base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Clean single crystal nickel base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Clean single crystal nickel base superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1454876