ABSTRACT:
A nickel base superalloy composition consisting essentially of, in weight %, 9.3-10.0% Co, 6.4-6.8% Cr, 0.5-0.7% Mo, 6.2-6.6% W, 6.3-6.7% Ta, 5.45-5.75% Al, 0.8-1.2% Ti, 0.07-0.12% Hf, 2.8-3.2% Re, and balance essentially Ni wherein a carbon concentration of about 0.01 to about 0.08 weight % is provided for improving the cleanliness of a single crystal investment casting produced therefrom.

REFERENCES:
patent: 3567526 (1971-03-01), Gell et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4402772 (1983-09-01), Duhl et al.
patent: 4643782 (1987-02-01), Harris et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 4801513 (1989-01-01), Duhl et al.
patent: 5069873 (1991-12-01), Harris et al.
patent: 5100484 (1992-03-01), Wukusick et al.
patent: 5240518 (1993-08-01), Wortman et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Clean single crystal nickel base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Clean single crystal nickel base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Clean single crystal nickel base superalloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1053879

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.