Alloys or metallic compositions – Nickel base – Aluminum containing
Patent
1981-12-30
1984-07-24
Dean, R.
Alloys or metallic compositions
Nickel base
Aluminum containing
75246, C22C 1903
Patent
active
044617410
ABSTRACT:
Rapidly solidified chromium and cobalt free superalloy powders are described. The compositions of the alloys are as follows:
REFERENCES:
patent: 4297135 (1981-10-01), Giessen et al.
patent: 4359352 (1982-11-01), Ray et al.
Allied Corporation
Dean R.
Fuchs Gerhard H,.
Hampilos Gus T.
Weins Michael J.
LandOfFree
Chromium and cobalt free nickel base superalloy powder does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Chromium and cobalt free nickel base superalloy powder, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Chromium and cobalt free nickel base superalloy powder will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-97646