ABSTRACT:
The efficiency of chromium utilization in chrome tanning of hides to make leather is greatly improved by performing the preliminary neutralization of the acid tanning liquor in the presence of an aldehydo or keto acid, before conventional subsequent neutralization with an alkali aluminum silicate. Most preferably, a combination of glyoxylic acid and magnesium oxide is used for the preliminary neutralization.

REFERENCES:
patent: 4272242 (1981-06-01), Plapper et al.
patent: 4715861 (1987-12-01), Lotz et al.
Das Leder, 26, 21-31 (1975); Das Leder, 34, 89-93 (1983).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Chrome tanning of leather with reduced waste of chromium does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Chrome tanning of leather with reduced waste of chromium, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Chrome tanning of leather with reduced waste of chromium will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1888226

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.