ABSTRACT:
Pretreatment of coal by devolatization at temperatures ranging from about 420.degree. C. to about 450.degree. C. for from about 10 minutes to about 30 minutes before leaching with molten caustic leads to a significant reduction in carbonate formation, greatly reducing the cost of cleaning coal on a per ton basis.

REFERENCES:
patent: 28543 (1860-05-01), Nock
patent: 3759673 (1973-09-01), Whitten et al.
patent: 4055400 (1977-10-01), Stambaugh et al.
patent: 4152120 (1979-05-01), Zavitsanos et al.
patent: 4384536 (1983-05-01), Biswas
patent: 4479804 (1984-10-01), Chen et al.
patent: 4497636 (1985-02-01), Aida et al.
patent: 4545891 (1985-10-01), Meyers et al.
patent: 4661118 (1987-04-01), Thorpe et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Chemical cleaning of coal by molten caustic leaching after pretr does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Chemical cleaning of coal by molten caustic leaching after pretr, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Chemical cleaning of coal by molten caustic leaching after pretr will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2415784

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.