ABSTRACT:
The resistance to internal charring of molded styrene-butadiene latex foam rubber when exposed to a lit cigarette is improved by incorporating from about 10 to 30 parts by dry weight, per hundred parts by dry weight of latex of a compound selected from the group consisting of an organic phosphate of the formula ##STR1## wherein R is a C.sub.6-12 alkyl radical or a phenyl radical, which is unsubstituted or substituted by a C.sub.1-4 alkyl radical, butyl benzyl phthalate, and a mixture thereof.
REFERENCES:
patent: 3699041 (1972-10-01), Sanderford et al.
patent: 4228245 (1980-10-01), Morgan et al.
Condensed Chemical Dictionary, 5th Ed., Reinhold, N.Y., (1956), p. 48.
Longuet Michel
Oberle Patrick
Walker David
Cockeram Herbert S.
Polysar International S.A.
LandOfFree
Char resistant foams does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Char resistant foams, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Char resistant foams will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2002053