ABSTRACT:
This invention concerns an improvement in cast iron material and chilled iron material. The cast iron material has a C.E. value of not more than 4.3 in which cerium is added in the form of a mischmetal upon casting to a cerium content of from 0.005 to 0.035 wt %. The chilled cast iron article has a chilled layer formed by remelting at least a portion of the surface of the cast iron of a predetermined shape composed of the above-mentioned cast iron by a high density energy source such as tungsten inert gas (TIG) arc, laser or electron beam.

REFERENCES:
patent: 4000011 (1976-12-01), Sato et al.
patent: 4450019 (1984-05-01), Satou et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Cast iron making by cerium addition does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Cast iron making by cerium addition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Cast iron making by cerium addition will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-205511

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.