ABSTRACT:
Monocarbide reinforced nickel-base eutectic superalloys which are particularly characterized by improved resistance to the formation of surface nucleated carbides and are, therefore, especially suited for making unidirectionally solidified anisotropic metallic bodies in the form of vanes and rotating blades for aircraft gas turbine engines are provided.
REFERENCES:
patent: 4292076 (1981-09-01), Gigliotti et al.
Gigliotti, Jr. Michael F. X.
Jackson Melvin R.
Yang Swe-Wong
Davis Jr. James C.
Dean R.
General Electric Company
Rochford Paul E.
Webb II Paul R.
LandOfFree
Carbide reinforced nickel-base superalloy eutectics having impro does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Carbide reinforced nickel-base superalloy eutectics having impro, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Carbide reinforced nickel-base superalloy eutectics having impro will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2106964