ABSTRACT:
In accordance with the invention, there is a battery defect detection method comprising applying a current ramp to a battery; determining a first time (t1) when a current of the battery reaches a maximum current (Ipeak), and determining a second time (t2) when a terminal voltage of the battery reaches a maximum voltage (Vpeak). The method also includes determining a differential (d), wherein (d)=/(t1)−(t2)/, and wherein (d) corresponds to a magnitude of defects in the battery.
REFERENCES:
patent: 4433294 (1984-02-01), Windebank
patent: 4745349 (1988-05-01), Palanisamy et al.
patent: 5049803 (1991-09-01), Palanisamy
patent: 5160880 (1992-11-01), Palanisamy
patent: 5644209 (1997-07-01), Chabbert et al.
patent: 5808447 (1998-09-01), Hagino
patent: 5926008 (1999-07-01), Palanisamy et al.
patent: 6094051 (2000-07-01), Palanisamy et al.
patent: 7076375 (2006-07-01), Raichle et al.
patent: 7078879 (2006-07-01), Makhija
patent: 7148657 (2006-12-01), Raichle et al.
patent: 2002/0193953 (2002-12-01), Hoenig et al.
patent: 2003/0006735 (2003-01-01), Kawakami et al.
patent: 2004/0160214 (2004-08-01), Blair et al.
patent: 1167988 (2002-01-01), None
International Search Report dated Jul. 6, 2006.
Atehortua Hector M.
Hoenig Steven
Palanisamy Thirumalai G.
Singh Harmohan N.
Honeywell International , Inc.
Oral Caglar Esq.
Tran Nguyen
Vu Bao Q.
LandOfFree
Capacity degredation in a lead acid battery method and... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Capacity degredation in a lead acid battery method and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Capacity degredation in a lead acid battery method and... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3935243