ABSTRACT:
Nickel stampers used for the molding of capacitive electronic discs are treated prior to use in the molding process by heating the stamper in the presence of an oxygen containing gas, at a temperature from about 220.degree. C. to about 300.degree. C. for 2 to 5 hours until a continuous protective oxide layer approximately 10-40 angstroms thick is formed on the surface of the stamper.

REFERENCES:
patent: 3909517 (1975-09-01), Clemens
patent: 4004080 (1977-01-01), Vossen, Jr. et al.
patent: 4057831 (1977-11-01), Jacobs et al.
patent: 4077051 (1978-02-01), Vossen, Jr.
patent: 4189331 (1980-02-01), Roy
"Tarnishing of Nickel in Air at Temperatures from 23.degree. to 200.degree. C. and Relative Humidities from Ambient to 95%" by S. H. Kulpa and R. P. Frankenthal, Electrochemical Society Solid-State Science and Technology, Oct. 1977.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Capacitance electronic disc stamper having improved stain resist does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Capacitance electronic disc stamper having improved stain resist, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Capacitance electronic disc stamper having improved stain resist will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-588322

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.