ABSTRACT:
In the production of reactive form coke of the sort described in Work et al., U.S. Pat. Nos. 3,140,241, 3,140,242 and 3,184,293, where a low-temperature reactive coal calcinate is mixed with a binder and formed into shapes which are cured in an oxygen-containing atmosphere and then calcined, the use of high-temperature coke oven pitch as binder for the briquettes is made possible by adding to the calcinate, before mixing with the binder, at least about 3.0% by weight of water based on the weight of calcinate.
REFERENCES:
patent: 3140241 (1964-07-01), Work
patent: 3623999 (1971-11-01), Juntgen
patent: 3661719 (1972-05-01), Kelmar
FMC Corporation
Mullen Martin G.
Yudkoff Norman
LandOfFree
Briquetting of reactive coal calcinate with high-temperature cok does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Briquetting of reactive coal calcinate with high-temperature cok, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Briquetting of reactive coal calcinate with high-temperature cok will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-377831