ABSTRACT:
A method for brightening a natural calcitic ore by removal of discoloring contaminants. The ore is crushed and formed into an aqueous slurry, which slurry is then coarse-milled to produce a product wherein no more than 1 percent of the particulate matter is +325 mesh. This coarse-milled product is then subjected to a further, wet-milling step, to alter the particulate such that at least 70 percent of the particles are less than 2 microns, thereby liberating substantial quantities of the discoloring contaminants. The liberated impurities are thereupon separated from the slurry by flotation and/or by subjecting the slurry to a high intensity magnetic field.

REFERENCES:
patent: 2287440 (1942-06-01), McCleary
patent: 3307790 (1967-03-01), Cohn et al.
patent: 3512722 (1970-05-01), Hall
patent: 3604634 (1971-09-01), Windle
patent: 3627678 (1971-12-01), Marston et al.
patent: 3819515 (1974-06-01), Allen

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Brightening of natural calcitic ores does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Brightening of natural calcitic ores, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Brightening of natural calcitic ores will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1022727

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.