Brazing composition and brazing method for superalloys

Metal fusion bonding – Process – Diffusion type

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C228S248100, C228S245000, C228S234100, C228S233100

Reexamination Certificate

active

07946471

ABSTRACT:
A brazing composition for the brazing of superalloys including a base material with at least one initial phase is provided. The initial phase has a solidus temperature that is below the solidus temperature of the base material and, above a certain temperature, forms with the base material and/or with at least one further initial phase at least one resultant phase, the solidus temperature of which is higher that the solidus temperature of the initial phases. Heat treatment takes place in two stages, wherein the temperature of the second heat treatment is preferably 800-1200° C. The brazing composition may likewise be of the type MCrAlX, and the power particles of the initial phase may be in the form of nanoparticles.

REFERENCES:
patent: 4507264 (1985-03-01), Stern
patent: 4914794 (1990-04-01), Strangman
patent: 5040718 (1991-08-01), Lee et al.
patent: 6024792 (2000-02-01), Kurz et al.
patent: 6613123 (2003-09-01), Corbin et al.
patent: 2004/0050913 (2004-03-01), Philip
patent: 0412397 (1991-02-01), None
patent: 0486489 (1992-05-01), None
patent: 0786017 (1997-07-01), None
patent: 0892090 (1999-01-01), None
patent: 1204776 (2002-05-01), None
patent: 1 258 545 (2002-11-01), None
patent: 1306454 (2003-05-01), None
patent: 1319729 (2003-06-01), None
patent: 1341639 (2003-09-01), None
patent: 62156095 (1987-07-01), None
patent: WO 96/19314 (1996-06-01), None
patent: WO 99/67435 (1999-12-01), None
patent: WO 00/44949 (2000-08-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Brazing composition and brazing method for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Brazing composition and brazing method for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Brazing composition and brazing method for superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2681901

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.