ABSTRACT:
Polyethylene resins having improved environmental stress crack resistance, stiffness and impact resistance is made by a process comprising feeding both a chromium oxide catalyst and a silyl chromium catalyst into a polymerization reactor. The chromium oxide catalyst and the silyl chromium catalyst are on separate supports. The chromium oxide catalyst is 25–50 weight percent and the silyl chromium catalyst is 50–75 weight percent of the total weight of catalyst. The catalysts may be added separately or as a single mixture.

REFERENCES:
patent: 2825721 (1958-03-01), Hogan et al.
patent: 3023203 (1962-02-01), Dye
patent: 3324095 (1967-06-01), Carrick et al.
patent: 3324101 (1967-06-01), Baker et al.
patent: 3622251 (1971-11-01), Allen
patent: 3687920 (1972-08-01), Johnson
patent: 3704287 (1972-11-01), Johnson
patent: 3709853 (1973-01-01), Karapinka
patent: 3798202 (1974-03-01), Nasser, Jr.
patent: 3959178 (1976-05-01), Hogan
patent: 4011382 (1977-03-01), Levine et al.
patent: 4025707 (1977-05-01), Hogan
patent: 4100105 (1978-07-01), Levine et al.
patent: 4115639 (1978-09-01), Brown et al.
patent: 4325839 (1982-04-01), McDaniel
patent: 4369295 (1983-01-01), McDaniel
patent: 4528790 (1985-07-01), Lo et al.
patent: 4994534 (1991-02-01), Rhee et al.
patent: 5034364 (1991-07-01), Kral et al.
patent: 5169816 (1992-12-01), Dawkins
patent: 5198400 (1993-03-01), Katzen et al.
patent: 5310834 (1994-05-01), Katzen et al.
patent: 5408015 (1995-04-01), Hsieh et al.
patent: 5459203 (1995-10-01), Geerts et al.
patent: 5462999 (1995-10-01), Griffin et al.
patent: 5527752 (1996-06-01), Reichle et al.
patent: 5527867 (1996-06-01), Bergmeister
patent: 5543376 (1996-08-01), Bergmeister
patent: 5624877 (1997-04-01), Bergmeister et al.
patent: 5648439 (1997-07-01), Bergmeister et al.
patent: 5866661 (1999-02-01), Benham et al.
patent: 5922818 (1999-07-01), Morterol
patent: 6022933 (2000-02-01), Wright et al.
patent: 6201078 (2001-03-01), Breulet et al.
patent: 6291602 (2001-09-01), Koch et al.
patent: 6335411 (2002-01-01), Koch et al.
patent: 2004/0167015 (2004-08-01), Cann et al.
patent: 789870 (1973-04-01), None
patent: 0291824 (1994-04-01), None
patent: 0591968 (1997-07-01), None
patent: 0647661 (1998-03-01), None
patent: 92/17511 (1992-10-01), None
patent: 96/21684 (1996-07-01), None
patent: 96/27621 (1996-09-01), None
patent: 97/27225 (1997-07-01), None
patent: 99/45038 (1999-09-01), None
patent: 99/52951 (1999-10-01), None
patent: 99/65949 (1999-12-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Blow molding resins with improved ESCR does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Blow molding resins with improved ESCR, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Blow molding resins with improved ESCR will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3585663

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.