ABSTRACT:

BACKGROUND OF THE INVENTION
The invention relates to a fuel cell stack with connecting elements for the fuel cells of the stack and also to a manufacturing method.
A fuel cell includes a cathode, an electrolyte as well as an anode. An oxidation medium such as air is supplied to the cathode and a fuel such as hydrogen is supplied to the anode.
Various types of fuel cells are known for example the SOFC-fuel cell disclosed in the printed publication DE 44 30 958 C1 and the PEM fuel cell disclosed in the printed publication DE 195 31 952 C1.
The SOFC-fuel cell is also called high-temperature fuel cell since it has an operating temperature of up to 1000° C. In the presence of an oxidation medium, oxygen ions are formed at the cathode of a high-temperature fuel cell. The oxygen ions pass through the electrolyte and recombine at the anode side with the hydrogen of the fuel to form water. During the recombination electrons are released whereby electric energy is generated.
The operating temperature of a PEM fuel cell is at about 80° C. In the presence of the fuel, protons are formed at the anode of a PEM fuel cell by means of a catalyst. The protons pass through the electrolyte and combine at the cathode side with the oxygen of the oxidation means to form water. During this process, electrons are released whereby electric energy is generated. For obtaining a large electric power output, generally several fuel cells are electrically and mechanically interconnected by connecting elements. An example of such a connecting element is the bi-polar plate disclosed in DE 44 10 711 C1. With the aid of bi-polar plates fuel cells can be arranged electrically in series and can be placed on top of one another. Such an arrangement is called a fuel cell stack.
As fuel methane or methanol, among others, can be used. The fuels mentioned are converted, by reformation or oxidation among others, to hydrogen or a hydrogen-rich gas.
It is known from the printed publication DE 195 198 47 C1 to reform fuel such as a methane internally, that is, directly at the anode of an SOFC fuel cell. A methane-steam reformation reaction is a highly endothermal reaction (&Dgr;H=227.5 kJ/mol at 1000° C.) and extracts a corresponding amount of heat from the surrounding area. The reaction rate of the reformation reaction is generally very high in comparison with the subsequent electrochemical reaction. In an internal reformation, the reformation reaction may be completed already within a distance of 10 mm from the gas entrance into the anode chamber (the chamber in which the anode is disposed). The heat required within such a short distance cannot be sufficiently supplied by the essentially slower electrochemical reaction so that, with internal reformation, there is always a temperature collapse. This results in uneven temperature distributions and consequently destructive thermal tensions.
In order to mitigate this problem, in accordance with the printed publication DE 195 198 47 C1, the catalyst concentrations in the anode chamber are suitably reduced so that the methane-steam reformation reaction occurs in a delayed fashion.
In the German Patent application with the official No. 197 10 345.6-45, it is described that a glass-containing paste is to be disposed between an electrode of a high temperature fuel cell and the adjacent bi-polar plate in order to reduce contact problems resulting from uneven surfaces.
From the printed publication DE 195 47 700 A1, it is known to arranged electrode spaces within a self-supporting electrode consisting of a cermet. In this way, the flow path of an operating medium from the electrode chamber to the catalytically active layer is to be kept short.
It is the object of the present invention to provide an inexpensive simple connecting element with which contact problems with an adjacent electrode are reduced. It is a further object of the invention to provide a method of producing a stack of fuel cells, which includes the connecting element.
SUMMARY OF THE INVENTION
In a fuel cell stack including several fuel cells each comprising a cathode, an anode and an electrolyte layer disposed between the anode and the cathode, wherein the anode includes a catalyst for the reforming or for the oxidation of fuel and the fuel cells are electrically and mechanically interconnected by connecting elements which consist of a metal or metal alloy. The connecting elements include each a porous wall on which the anode is formed so as to be in close contact with the respective connecting element.
The connecting element consists—except for welding or soldering connections—essentially of a metal or of related metals, for example, of metals with comparable physical and chemical properties.
An anode is produced on the porous layer of the connecting element. For example, it is produced by pouring onto the porous layer a suspension, which contains the electrode material in the form of a powder. The electrode material is deposited on the connecting element as a layer. It is then dried and sintered.
Because the anode is produced on the connecting element, there are no contact problems resulting from uneven surfaces.
The porous separation wall inhibits the diffusion of operating media to the catalytically active layer. Only a part of the fuel in the entrance area of the respective anode chamber reaches directly the anode. As a result, the fuel to be reformed is evenly distributed in the anode chamber. Localized cooling is avoided in this way.
The porosity of the porous separation wall of the connecting element is preferably 20 to 60% in order to achieve the effect mentioned before.
In an advantageous embodiment of the invention, the connecting element consists particularly of an iron-chromium alloy, for example, of the alloy having the material number 1,4742. Such a connecting element can be employed at high temperatures of more than 500° C. The connecting element may be composed of different building components, which are soldered or welded together. Such a connection is more stable and easier to produce than a connection by a glass containing paste mentioned earlier.
In another advantageous embodiment, the anode consists of cermet so that it can be employed at high temperatures of over 500° C.
Producing an anode on the porous wall means that a preliminary body of the electrode is deposited on the porous wall and that the anode is formed from the preliminary body by subsequent treatment of the preliminary body.


REFERENCES:
patent: 5034288 (1991-07-01), Bossel
patent: 5643690 (1997-07-01), Tateishi et al.
patent: 41 20 359 (1992-01-01), None
patent: 0 108 467 (1984-05-01), None
patent: 0 297 315 (1989-01-01), None
patent: 0 378 812 (1990-07-01), None
patent: 0 817 297 (1998-01-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Bipolar plate with porous wall for a fuel cell stack does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Bipolar plate with porous wall for a fuel cell stack, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Bipolar plate with porous wall for a fuel cell stack will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3025616

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.