ABSTRACT:
Apparatus is disclosed for measuring creep stiffness of a specimen, for example, asphalt cement, or other viscoelastic material, having a flexural modulus greater than approximately 1,000 psi. The specimen and the lower part of a loading mechanism are submerged in a constant temperature coolant thereby providing buoyant support to the specimen, preventing it from deflecting under its own weight, as well as providing means for controlling the test temperature. The coolant temperature is maintained to within approximately +/-0.1.degree. C. of a desired temperature. The specimen, having known dimensions, is supported within the coolant on two spaced apart support members. A loading head actuated by an air bearing/pneumatic piston mechanism engages the specimen midway between the two support members. The deflection of the specimen is measured with an LVDT and the load imparted to the specimen by a load cell provided under at least one of the specimen support members. In order to prevent the buildup of frost on the apparatus, those components which extend from the air into the coolant are composed of low conductive material such as polymethylmethacrylate.

REFERENCES:
patent: 2404584 (1946-07-01), Liska et al.
patent: 2506048 (1950-05-01), Van Den Akker
patent: 2670624 (1954-03-01), Faris, Jr. et al.
patent: 3323356 (1967-06-01), Arias
patent: 3324714 (1967-06-01), Simon et al.
patent: 3640127 (1972-02-01), Meissner
patent: 3831438 (1974-08-01), Schmidt
patent: 3881346 (1975-05-01), Scheucher
patent: 4033181 (1977-07-01), Oeser
patent: 4036048 (1977-07-01), Webster
patent: 4096741 (1978-06-01), Sternstein
patent: 4179004 (1979-12-01), Ebbinge
patent: 4213349 (1980-07-01), Miura
patent: 4266424 (1981-05-01), Muenstedt
patent: 4478086 (1984-10-01), Gram
patent: 4478093 (1984-10-01), Valadier
patent: 4535636 (1985-08-01), Blacksburn et al.
patent: 4589288 (1986-05-01), Porter et al.
patent: 4679441 (1987-07-01), Johnson et al.
patent: 4721000 (1988-01-01), Scanlon
patent: 4730498 (1988-03-01), Blanch
patent: 4763529 (1988-08-01), Leonard et al.
patent: 4942768 (1990-07-01), McRae
patent: 4982609 (1991-01-01), Talley III

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Bending beam creep test device with piston having a gas bearing does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Bending beam creep test device with piston having a gas bearing, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Bending beam creep test device with piston having a gas bearing will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2197323

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.