ABSTRACT:
A rough and porous coating is applied by spraying and metallurgically bonding to a bearing member. The coating is preferably of a strong and thermally conductive material, such as aluminum-bronze, with the coating having interstices, such as cavities, undercuts, and craters to provide a porous material. An adhesive-solid lubricant formulation is then applied to the coating. The adhesive-solid lubricant formulation fills the coating interstices. The adhesive-solid lubricant formulation is cured for the required time at the required temperature to form a low-friction bearing surface layer.

REFERENCES:
patent: 3206264 (1965-09-01), Dalzell et al.
patent: 3266123 (1966-08-01), McCloskey

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Bearing element does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Bearing element, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Bearing element will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1832453

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.