ABSTRACT:
Disclosed is an improved process for affecting preparation of resin particles by a bead polymerization reaction which for example comprises (1) providing a solution mixture of water, suspension agent, and surfactant; (2) adding thereto while stirring a monomer component, a low molecular weight wax, and a polymerization initiator; (3) affecting polymerization of the monomer by heating the resulting solution at a temperature of from about 90 degrees Centigrade to about 120 degrees Centigrade; and (4) separating the resulting polymer from the reaction mixture.

REFERENCES:
patent: 2948710 (1960-08-01), D'Alelio et al.
patent: 3338991 (1967-08-01), Insalaco et al.
patent: 3379664 (1968-04-01), Wiley
patent: 3391082 (1968-07-01), Maclay
patent: 3647723 (1972-03-01), Mysik et al.
patent: 3950290 (1976-04-01), Drury, Jr. et al.
patent: 3989649 (1976-11-01), Kaiho et al.
patent: 3997488 (1976-12-01), Tsubuko et al.
patent: 4081391 (1978-03-01), Tsubuko et al.
patent: 4100087 (1978-07-01), Takayama et al.
patent: 4176107 (1979-11-01), Buckman et al.
patent: 4211684 (1980-07-01), Koyama et al.
patent: 4243717 (1981-01-01), Gahmig
patent: 4385107 (1983-05-01), Tanaka et al.
patent: 4433029 (1984-02-01), Senda et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Bead polymerization process for toner resin compositions does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Bead polymerization process for toner resin compositions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Bead polymerization process for toner resin compositions will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-700235

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.