ABSTRACT:
The invention comprises a structural member formed from iron alloyed with 0.15% to 0.20% carbon, 1.00% to 1.80% manganese, 1.00% to 1.60% silicon, 1.50% to 2.50% chromium, 2.50% to 3.50% nickel, 0.40% to 0.70% molybdenum and 0.0025% to 0.0005% boron, all by weight. Preferably, alloy is subjected to a two-level thermal processing to confer a bainitic structure to the steel. Also preferably, the structural member is a frog for a railway track switch.

REFERENCES:
patent: 5382307 (1995-01-01), Kageyama et al.
patent: 5759299 (1998-06-01), Yokoyama et al.
patent: 5879474 (1999-03-01), Bhadeshia et al.
patent: 6254696 (2001-07-01), Ueda et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Bainitic steel alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Bainitic steel alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Bainitic steel alloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3984185

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.