ABSTRACT:
A method of using an apparatus for the automatic lacing (drawing) of hairpin tubes through the holes of a heat exchanger fin stack includes using a plurality of identical extendable guide rods, each positioned in approximate alignment to engage an open end of a respective heat exchanger tube which is positioned adjacent to a respective fin stack hole. The plurality of guide rods are extended in unison through the holes of the heat exchanger fin stack to positions within the open ends of the hairpin tubes. A self aligning knurl structure on each guide rod lead end is expanded to engage the respective I.D. of a respective hairpin tube. The guide rods are then retracted in unison pulling the tubes through the fin stack holes. A self regulating pressure mechanism assures that the pressure exerted by an expanding knurl end is within a predetermined range. Once the tubes have been laced, the knurl structures are collapsed and the guide rods withdraw from the tubes.
REFERENCES:
patent: 3815672 (1974-06-01), Bullard et al.
patent: 4519121 (1985-05-01), Yokosawa
patent: 4601088 (1986-07-01), Kopczynski
patent: 4734969 (1988-04-01), Currier et al.
patent: 4839950 (1989-06-01), Stroup
patent: 4970770 (1990-11-01), Sansson et al.
patent: 5154679 (1992-10-01), Fuller et al.
patent: 5267610 (1993-12-01), Culbert
Cuda Irene
Gore Gregory J.
LandOfFree
Automatic hairpinlacing process does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Automatic hairpinlacing process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Automatic hairpinlacing process will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2134050