ABSTRACT:
Contaminated oily soil is used as a component in a cold mix asphaltic concrete. The soil is mixed with asphalt roof cuttings containing fibers and mineral aggregate to form a mixture. This mixture is coated with a cold mix emulsion to form an asphaltic concrete. The hydrocarbons do not leach from the set concrete.

REFERENCES:
patent: 1778461 (1930-10-01), Nicholson
patent: 2323435 (1940-05-01), Wiseblood
patent: 2750297 (1956-06-01), Doherty
patent: 4373961 (1983-02-01), Stone
patent: 4706893 (1987-11-01), Brock
patent: 4738996 (1988-04-01), Vonk et al.
patent: 5173115 (1992-12-01), Glynn, Jr. et al.
"Petroleum Contaminated Soils", Kostecki et al., vol. I, 1989, pp. 191-199.
"Making Use of Contaminated Soil", Czarnecki, Civil Engineering Dec. 1988.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Asphaltic concrete product and a method for the fixation of cont does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Asphaltic concrete product and a method for the fixation of cont, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Asphaltic concrete product and a method for the fixation of cont will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1327133

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.