Aqueous polymer dispersions as binders for elastic, nonblocking

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – At least one aryl ring which is part of a fused or bridged...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

523201, 524521, 524522, 526201, C08F 222, C08F 224

Patent

active

06005042&

ABSTRACT:
A polymer dispersion having a minimum film-forming temperature in the range from 0 to 40.degree. C., which is useful in coating compositions for substrates, in the form of varnishes or gloss paints, is obtained by stepwise emulsion polymerization, which includes polymerizing, onto a first stage having the monomer composition I comprising: from 50 to 68.5% by weight of soft monomers A whose homopolymers have a glass transition temperature (T.sub.g) below 0.degree. C.; from 30 to 50% by weight of hard monomers B whose homopolymers have a glass transition temperature (T.sub.g) above 65.degree. C.; from 0.5 to 5% by weight of .alpha.,.beta.-unsaturated carboxylic acids and/or carboxamides C which are copolymerizable with A and B; from 1 to 7.5% by weight of ethylenically unsaturated monomers D containing keto groups; and from 0 to 10% by weight of other ethylenically unsaturated monomers E which do not contain a nitrogen atom, where the weight percentages in each case are based on the overall amount of the polymer of the first stage, a second stage having the monomer composition II comprising: from 5 to 45% by weight of soft monomers A whose homopolymers have a glass transition temperature (T.sub.g) below 0.degree. C.; from 65 to 95% by weight of hard monomers B whose homopolymers have a glass transition temperature (T.sub.g) above 65.degree. C.; from 0 to 4% by weight of .alpha.,.beta.-unsaturated carboxylic acids and/or carboxamides C which are copolymerizable with A and B; from 0 to 5% by weight of ethylenically unsaturated monomers D containing keto groups; and from 0 to 10% by weight of other ethylenically unsaturated monomers E which do not contain a nitrogen atom, where the weight percentages in each case are based on the overall amount of the polymer of the second stage, in a weight ratio of the monomer composition I to the monomer composition II of from 50:50 to 75:25.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Aqueous polymer dispersions as binders for elastic, nonblocking does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Aqueous polymer dispersions as binders for elastic, nonblocking , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aqueous polymer dispersions as binders for elastic, nonblocking will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-506001

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.