ABSTRACT:
This foaming system includes a foaming agent solution and a resin solution. The foaming agent includes the relative amounts of 15 to 30 parts by weight of a salt of an alkyl diphenyl oxide sulfonate, 10 to 25 parts of 85% phosphoric acid and 15 to 25 parts urea, all in an aqueous solution. The resin solution includes a resin prepared by reacting 1 to 2.4 mols of formaldehyde per 1 mol of urea, 6.5 to 500 mmols polyethylene glycol as foam charring agent, 0.3 to 1.2 mmols of calcium carbonate as uniform foam cell size agent, 3 to 310 mmols of dicyandiamide as foam hydrolysis resistance agent, 2 to 30 mmols of sodium bromide as foam aging agent, and sufficient water to make a 35 to 45% solution. In preparing the foam, one part by weight of the foaming agent solution of about 5% solids concentration is aerated and then 1.0 to 1.5 parts by weight of the resin solution is sprayed thereon to obtain foam with an average linear shrinkage of about 0.25%.
REFERENCES:
patent: 3997467 (1976-12-01), Jederstrom
patent: 4225680 (1980-09-01), Williams
Borden Inc.
Helfin Bernard
Maskas George P.
Millard Sidney
Van Wyck Kenneth P.
LandOfFree
Aqueous foaming agent solution does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Aqueous foaming agent solution, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aqueous foaming agent solution will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1530571