Chemistry: electrical and wave energy – Processes and products
Patent
1989-12-22
1990-08-28
Tufariello, T. M.
Chemistry: electrical and wave energy
Processes and products
204 351, C25D 548, C25D 706
Patent
active
049522850
ABSTRACT:
A method of imparting tarnish and corrosion resistance to a copper or copper alloy foil, particularly wrought foil having one surface roughened by the application of nodules or dendrites. The foil is treated with an aqueous solution of chromic acid and sulfuric acid. The foil may then be rinsed in a basic solution having a pH greater than 8 and then dried.
REFERENCES:
patent: 2030601 (1936-02-01), McDonald
patent: 2412543 (1943-12-01), Tanner
patent: 2418608 (1947-04-01), Thompson
patent: 2647865 (1953-08-01), Freud
patent: 3625844 (1971-12-01), McKean
patent: 3677828 (1972-07-01), Caule
patent: 3716427 (1973-02-01), Caule
patent: 3764400 (1973-10-01), Caule
patent: 3853716 (1974-12-01), Yates et al.
patent: 4131517 (1978-12-01), Mitsuo et al.
patent: 4387006 (1983-06-01), Kajiwara et al.
patent: 4432846 (1984-02-01), Honeycutt, III
patent: 4468293 (1984-08-01), Polan et al.
patent: 4515671 (1985-05-01), Polan et al.
patent: 4549950 (1985-10-01), Polan et al.
patent: 4647315 (1987-03-01), Parthasarathi et al.
U.S. Patent Application Ser. No. 333,212 filed Apr. 5, 1989, L. Lifun and N. W. Polan.
U.S. Patent Application Ser. No. 333,210 filed Apr. 5, 1989, L. Lifun and N. W. Polan.
Chao Chung-Yao
Lin Lifun
Polan Ned W.
Kieser H. Samuel
Olin Corporation
Tufariello T. M.
LandOfFree
Anti-tarnish treatment of metal foil does not yet have a rating. At this time, there are no reviews or comments for this patent.