ABSTRACT:
A process for producing aluminum in which alumina is decomposed electrolytically to aluminum metal in an electrolyte bath between an anode and a cathodic interface formed between aluminum metal and the electrolyte bath. The bath consists essentially of Al.sub.2 O.sub.3, NaF, and AlF.sub.3, and has a weight ratio NaF to AlF.sub.3 up to 1.1:1. During decomposition, the bath is maintained at an operating temperature greater than 40.degree.C above the cryolite liquidus temperature of the bath and effective for preventing bath crusting in interfacial areas between bath and aluminum metal.
REFERENCES:
patent: 2915443 (1959-12-01), Wallace et al.
Gadeau, Bull. Soc. Franc Electriciens, Ser. 6, Vol. VII, No. 74, pp. 540-544, 1947.
Antipin et al., Metallurgizdat, 1954, pp. 250, 251.
Rolin, Bull. Soc. Chim. de France, 1961, pp. 1112-1125.
Cochran C. Norman
Foster, Jr. Perry A.
Haupin Warren E.
Sleppy William C.
Aluminum Company of America
Edmundson F. C.
Sullivan Jr. Daniel A.
LandOfFree
Aluminum smelting temperature selection does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Aluminum smelting temperature selection, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminum smelting temperature selection will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1585360