Aluminum nitride sintered body, method for manufacturing the sam

Compositions: ceramic – Ceramic compositions – Refractory

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

428209, 428698, 428697, 428696, 428901, C04B 35581

Patent

active

054098696

ABSTRACT:
Disclosed is an aluminum nitride sintered body which has a high thermal conductivity and a high strength and which can be manufactured through low-temperature, short-time sintering. This aluminum nitride sintered body has an average grain size of aluminum nitride grains of 2 .mu.m or less, a thermal conductivity of 80 W/m.K or more, and a relative density of 98% or more.

REFERENCES:
patent: 4659611 (1987-04-01), Iwase et al.
patent: 4698320 (1987-10-01), Kasori et al.
patent: 4711861 (1987-12-01), Sawamura et al.
patent: 4719187 (1988-01-01), Bardhan et al.
patent: 4746637 (1988-05-01), Kasori et al.
patent: 4952535 (1990-08-01), Merkel
patent: 5063183 (1991-11-01), Taniguchi et al.
E. Ueno, et al., "Yogyo-kiso Toronkai Ko-enyo-shi shu", Jan. 22, 1986, p. 176.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Aluminum nitride sintered body, method for manufacturing the sam does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Aluminum nitride sintered body, method for manufacturing the sam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminum nitride sintered body, method for manufacturing the sam will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1567442

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.