ABSTRACT:
The invention provides a silicon carbide fiber carrying an aluminum nitride coating between about 1 and about 15 micrometers thick. The AlN coating serves as a debond layer which improves the fracture toughness of composite materials in which the coated fiber is a reinforcement phase.

REFERENCES:
patent: Re32843 (1989-01-01), Wei
patent: 2938807 (1960-05-01), Andersen
patent: 3205043 (1965-09-01), Taylor
patent: 3305372 (1967-02-01), Taylor
patent: 3492153 (1970-01-01), Ervin
patent: 3617437 (1971-11-01), Bagg et al.
patent: 3627519 (1971-12-01), Baker et al.
patent: 3649310 (1972-08-01), Yates
patent: 3736159 (1970-03-01), Gibson et al.
patent: 3765300 (1973-10-01), Taylor et al.
patent: 4097293 (1978-06-01), Komeyr et al.
patent: 4332755 (1982-06-01), Murata
patent: 4507224 (1985-03-01), Toibana et al.
patent: 4539298 (1985-09-01), Komeya et al.
patent: 4562040 (1985-12-01), Yamada et al.
patent: 4632794 (1986-12-01), Mori et al.
patent: 4642271 (1987-02-01), Rice
patent: 4735756 (1988-04-01), Rausch
patent: 4800064 (1989-01-01), Kemp, Jr. et al.
patent: 4820663 (1989-04-01), Mehrotra et al.
patent: 4876941 (1989-10-01), Barnes et al.
patent: 4929472 (1990-05-01), Sugihara et al.
patent: 4931242 (1990-06-01), Uchimura et al.
patent: 4944904 (1990-07-01), Singh et al.
patent: 5202059 (1993-04-01), Kennedy
patent: 5231061 (1993-07-01), Devore
patent: 5296311 (1994-03-01), McMurtry
patent: 5332619 (1994-07-01), Lacoste
F. Abbe and J. Chermant, Fiber-Matrix Bond Strength Characterization of Silicon Carbide-Silicon Carbide Materials, 1990, J. Am. Ceram Soc, 73[8]pp. 2573-2575.
P. G. Charalambides, Fiber Debonding in Residually Stressed Brittle Matrik Composites, 1990, J. Am. Ceram. Soc. 73 [6]pp. 1674-1680.
Shanti V. Nair, Crack-Wake Debonding and Toughness in Fiber-or Whisker-Reinforced Brittle-Matrix Composites, 1990, J. Am. Ceram Soc., 73[10]2839-47.
T. P. Weihs and W. D. Nix, Experimental Examination of the Push-Down Technique for Measuring the Sliding Resistance of Silicon Carbide Fibers in a Ceramic Matrix, 1991, J. Am. Ceram. Soc., 74[3]524-34.
T. P. Weihs et al., Correlating the Mechanical Properties of a Continuous Fiber-Reinforced Ceramic Matrix Composite to the Sliding Resistance of the Fibers, 1991, J. Am. Ceram. Soc, 74[3]535-40.
I. Teusel and C. Russel, Aluminium nitride coatings on silicon carbide fibres, prepared by pyrolysis of a polymeric precursor, 1990, Jour. of Materials Science (25) pp. 3531-3534.
P. F. Becher, Microstructural Design of Toughened Ceramics, 1991, J. Am. Ceram. Soc., 74[2]255-69.
Behrendt and Dacek, Progress in Reaction-Formed SiC Matrix Composites, 1990. NASA Hi Temp. Review. pp. 57-1 to 57-12.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Aluminum nitride-coated silicon carbide fiber does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Aluminum nitride-coated silicon carbide fiber, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminum nitride-coated silicon carbide fiber will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-308266

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.