Aluminum matrix composite wire

Stock material or miscellaneous articles – All metal or with adjacent metals – Laterally noncoextensive components

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C428S539500, C428S611000, C428S629000, C428S650000

Reexamination Certificate

active

06913838

ABSTRACT:
Aluminum matrix composite wire comprising ceramic fibers with a matrix of aluminum.

REFERENCES:
patent: 2883314 (1959-04-01), Martin
patent: 3098723 (1963-07-01), Micks
patent: 3294604 (1966-12-01), Feick, III
patent: 3547180 (1970-12-01), Cochran et al.
patent: 3631519 (1971-12-01), Hooshang
patent: 3795524 (1974-03-01), Sowman
patent: 3808015 (1974-04-01), Seufert
patent: 3813481 (1974-05-01), Adams
patent: 4012204 (1977-03-01), Riewald et al.
patent: 4047965 (1977-09-01), Karst et al.
patent: 4053011 (1977-10-01), Riewald et al.
patent: 4152149 (1979-05-01), Horikiri et al.
patent: 4341823 (1982-07-01), Sexton et al.
patent: 4450207 (1984-05-01), Donomoto et al.
patent: 4544610 (1985-10-01), Okamoto et al.
patent: 4590132 (1986-05-01), Dohnomoto et al.
patent: 4631793 (1986-12-01), Shintaku et al.
patent: 4649060 (1987-03-01), Ishikawa et al.
patent: 4751269 (1988-06-01), Bonk et al.
patent: 4757790 (1988-07-01), Ushio et al.
patent: 4779563 (1988-10-01), Ishikawa et al.
patent: 4818633 (1989-04-01), Dinwoodie et al.
patent: 4831707 (1989-05-01), Goddard et al.
patent: 4835340 (1989-05-01), Muz
patent: 4839238 (1989-06-01), Nakatani et al.
patent: 4877643 (1989-10-01), Ishikawa et al.
patent: 4929513 (1990-05-01), Kyono et al.
patent: 4954462 (1990-09-01), Wood et al.
patent: 4956523 (1990-09-01), Pawluk
patent: 4961990 (1990-10-01), Yamada et al.
patent: 5002836 (1991-03-01), Dinwoodie et al.
patent: 5126167 (1992-06-01), Matsuno et al.
patent: 5170015 (1992-12-01), Kudo et al.
patent: 5171942 (1992-12-01), Powers
patent: 5185299 (1993-02-01), Wood et al.
patent: 5435374 (1995-07-01), Fishkis et al.
patent: 5464949 (1995-11-01), Markovitz et al.
patent: 5501906 (1996-03-01), Deve
patent: 5518597 (1996-05-01), Storer et al.
patent: 5549770 (1996-08-01), Larker et al.
patent: 5554826 (1996-09-01), Gentry
patent: 5571296 (1996-11-01), Barber, Jr. et al.
patent: 6022914 (2000-02-01), Nowak et al.
patent: 6078010 (2000-06-01), Funahashi et al.
patent: 6180232 (2001-01-01), McCullough et al.
patent: 6245425 (2001-06-01), McCullough et al.
patent: 6329056 (2001-12-01), Deve et al.
patent: 6336495 (2002-01-01), McCullough et al.
patent: 6485796 (2002-11-01), Carpenter et al.
patent: 6559385 (2003-05-01), Johnson et al.
patent: 6692842 (2004-02-01), McCullough et al.
patent: 3822543 (1990-01-01), None
patent: 0 461 871 (1991-12-01), None
patent: 52-36274 (1977-09-01), None
patent: 3-129606 (1989-09-01), None
patent: 2-155129 (1990-06-01), None
patent: 3-71509 (1991-03-01), None
patent: 3-101004 (1991-04-01), None
patent: 3-101011 (1991-04-01), None
patent: 5-290632 (1992-04-01), None
patent: 4-44366 (1992-07-01), None
patent: 7-13056 (1995-01-01), None
patent: 7-105761 (1995-04-01), None
patent: 10-21758 (1998-01-01), None
patent: WO 97/00976 (1997-01-01), None
3M Product Brochure, “Continuous Ceramic Fiber Aluminum Matrix Composites,” 3M Metal Matrix Composite Project, St. Paul, Minnesota, date unknown but belived to be prior to filing of the priority application, 6 pages.
ASTM B 230/B 230M—99, “Standard Specification for Aluminum 1350-H19 Wire for Electrical Purposes,”Annual Book of ASTM Standards, vol. 02.03, (1999), pp. 100-104.
ASTM D 3379-75, “Standard Test Method for Tensile Strength and Young's Modulus for High-Modulus Single-Filament Materials,”Annual Book of ASTM Standards, vol. 08.01, (1989), pp. 128-131.
ASTM E 228-95, “Standard Test Method for Linear Thermal Expansion of Solid Materials with a Vitreous Silica Dilatometer,”Annual Book of ASTM Standards, vol. 08.01, (1995), pp. 70-76.
ASTM E 345-93, “Standard Test Methods of Tension Testing of Metallic Foil,”Annual Book of ASTM Standards, vol. 02.03, (1993), pp. 376-380.
Blucher et al., “A New Pressure Infiltration Process for Continous Production of Fiber Reinforced MMC Structural Elements,”30thInternational SAMPE Technical conference Proceedings, Oct, 20-24, 1998, pp. 442-455.
Cheng et al., “Preparation of Carbon Fibre Reinforced Aluminum via Ultrasonic Liquid Infiltration Technique,”Materials Science&Technology, vol. 9, (1993), pp. 609-614.
Costello, “Testing of a Wire Rope,” inTheory of Wire Rope, 2ndEdition, Chapter 6, Springer-Verlag, (1997), title page and pp. 72-85.
Davis et al., Eds., “Metals Handbook® Ninth Edition vol. 15 Casting,” ASM International, Metals Park, Ohio, date unknown but believed to be prior to filing date of the priority application, title page, publication page, pp. 238-241, 275, 281-282, 300-304, 372-373, 487-488, and 755-757.
Dupont Product Brochure, “Technical Data FP/Aluminum Composites,” date unknown but believed to be prior to filing date of the priority application, p. 81.
Electric Power Research Institute, “Structural Composite Cores for Overhead Power Transmission Conductors,”EM-5110, Research Project 2426-9, (1987), 39 pages.
Gigerenzer et al., “Drawing of Graphite Fiber Reinforced Aluminum Composites,”Failure Modes and Processing of Composites IV, eds., J.A. Cornie and F. W. Crossman, (1977), pp. 359-369.
Gigerener et al., “Hot Drawing of Fiber (Filoment) Reinforced Metal-Matrix Composites,”ICCM2, Proceedings of the 1978 International Conference on Composite Materials, Toronto, Canada, Apr. 16-20, 1978, title page and pp. 175-188.
Goddard et al., “Continuous Graphite Fiber MMCs,”Engineered Materials Handbook, vol. 1: Composites, ASM International, (1987) pp. 867-873.
Hunn, “MMC Overview—1985, ”SME Composites in Manufacturing 5, Technical Paper, Los Angeles, California, EM86-106, Jan. 13-16, 1986, 14 pages.
Isaacs et al., “Structure and Plasticity of Aluminum Reinforced with Continuous Alumina Fibers,”Proceedings of the 12thInternational Riso Symposium of Metallurgy and Materials Science: Metal Matrix Composites—Processing, Microstructure and Properties, (1991), pp. 399-404.
Kaiser Aluminum and Chemical ISales, Inc.,Casting Kaise Aluminum, “Pig and Ingot Product Data Casting Practices and Characteristics of Molten Aluminum,” Oakland, California, (1956), title page, publication page, and pp. 59-61.
Katzman, “Fiber Coatings for Composite Fabrication,”Materials&Manufacturing Processes, vol. 5(1), (1990), pp. 1-15.
Nippon Carbon Co. Ltd., “Development of Wire Composite (SiC Fibre “NICALON” Reinforced Aluminum Composite Materials,” (Internal Report), date unknown but believed to be prior to filing of the priority application, pp. 1-24.
Ozawa et al., “Development and Evaluation Characteristics of SiC Fiber Reinforced Aluminum Composite Wires for Transmission Line,”The Electricity Society Electronics and Energy Department Symposium, (1995), 6 pages and translation, 9 pages.
Ozawa et al., “Mechnical Characteristics of SiC Fiber Reinforced Aluminum Composite Material,”The Electicity Society National Symposium, (1995), 1 page and translation, 2 pages.
Ozawa et al., “Mechanical Characteristics of SiC Fiber Reinforced Composite Wire,”The Electricity Society National Symposium, (1996), 2 pages and translation, 3 pages.
Pan et al., “Application of Ultrasonic Infiltration in Metal Matrix Composites,”Key Engineering Materials, vols. 104-107, (1995), pp. 275-282.
Pan et al., “A Study of the Ultrasonic Technique Applied in Fabrication of SiC Fiber-Reinforced Aluminum Composites,”Journal of Material Research, vol. 10(3), (1995), pp. 596-601.
Ronald et al., “Advanced Materials to Fly High in NASP,”Advanced Materials&Processes, vol. 5, (1989), pp. 29-35.
Tokyo Rope Mfg. Co. Ltd., “Technical Data on CFCC,” (Internal Report), Tokyo, Japan date unknown but believed to be prior to filing date of the prioirty application, 45 pages.
Yasutomi et al., “Effects of the SiC/Al Interface Reaction of Fracture Behavior on a Composite Conductor Using SiC Fiber Reinforced Aluminum for Next Generation

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Aluminum matrix composite wire does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Aluminum matrix composite wire, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminum matrix composite wire will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3404007

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.