ABSTRACT:
A family of ductile, non-aggressive, low temperature brazing alloys, particularly suitable for brazing and diffusion-welding aluminum alloys, titanium alloys, beryllium alloys, boron-borsic-graphite composite structures to such alloys, diamond bonding and dissimilar metal joints of aluminum, titanium or steels. The family of aluminum base brazing alloys include, by weight, 0.1 to 5% magnesium, 0.1 to 5% rare earth, 4 to 15% silicon and an addition of 1 to 9% tin, 0.3 to 5% copper, 2 to 10% palladium, 1 to 6% gallium, 1 to 8% silver or 0.1 to 0.25% bismuth or strontium, with the balance aluminum. Where the addition is palladium, the silicon content may be 0 to 12%.

REFERENCES:
patent: 3440712 (1969-04-01), Stroup et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Aluminum base fluxless brazing alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Aluminum base fluxless brazing alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminum base fluxless brazing alloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1225752

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.