Stock material or miscellaneous articles – All metal or with adjacent metals – Having metal particles
Patent
1989-03-06
1990-06-12
Lechert, Jr., Stephen J.
Stock material or miscellaneous articles
All metal or with adjacent metals
Having metal particles
428615, 428652, 428660, 428663, 428678, 428220, 428457, 4289088, 419 8, 419 9, 419 30, 419 38, 427 34, 427250, B22F 704
Patent
active
049332392
ABSTRACT:
A protective coating system for superalloys is described. The coating is an active element enriched aluminide, and can be formed by aluminizing an overlay coated superalloy, wherein during the aluminizing process, aluminum diffuses completely through the overlay coating and into the substrate. The coating system exhibits desirable oxidation resistance and resistance to thermal fatigue cracking, due to the presence of oxygen active elements in the overlay.
REFERENCES:
patent: Re30995 (1982-07-01), Rairden, III
patent: Re31339 (1983-08-01), Dardi et al.
patent: Re32121 (1986-04-01), Gupta et al.
patent: 3129069 (1964-04-01), Hanink et al.
patent: 3594219 (1971-07-01), Maxwell et al.
patent: 3819338 (1974-06-01), Bungardt et al.
patent: 3869779 (1975-03-01), Gedwill et al.
patent: 3873347 (1975-03-01), Walker et al.
patent: 3874901 (1975-04-01), Rairden, III
patent: 3918139 (1975-11-01), Felten
patent: 3961098 (1976-06-01), Bessen
patent: 3961910 (1976-06-01), Baladjanian et al.
patent: 3979273 (1976-09-01), Panzera et al.
patent: 3999956 (1976-12-01), Stueber et al.
patent: 4005989 (1977-02-01), Preston
patent: 4024294 (1977-05-01), Rairden, III
patent: 4070507 (1978-01-01), Stueber et al.
patent: 4080486 (1978-03-01), Walker et al.
patent: 4101713 (1978-07-01), Hirsch et al.
patent: 4117179 (1978-09-01), Jackson et al.
patent: 4123594 (1978-10-01), Chang
patent: 4123595 (1978-10-01), Chang
patent: 4152223 (1979-05-01), Wallace et al.
patent: 4198442 (1980-04-01), Gupta et al.
patent: 4246323 (1981-01-01), Bornstein et al.
patent: 4371570 (1983-02-01), Goebel et al.
patent: 4382976 (1983-05-01), Restall
patent: 4714624 (1987-12-01), Naik
Metallurgical Coatings 1988, R. C. Krutenat (Ed), vol. 1, Elsevier Applied Science, pp. 61-74.
Gupta Dinesh K.
Olson Walter E.
Bhat Nina
Lechert Jr. Stephen J.
Rashid J. M.
United Technologies Corporation
LandOfFree
Aluminide coating for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Aluminide coating for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Aluminide coating for superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-616628