ABSTRACT:
An alumina-zirconia sintered body comprising 92 to 35% by weight of aluminum oxide and 8 to 65% by weight of zirconium oxide having mainly tetragonal system, and 0.2 to 5 parts by weight of silicon oxide per 100 parts by weight of the total of aluminum oxide and zirconium oxide, and having a relative density of 95% or more, has improved wear resistance and suitable for use in an impact grinder.
REFERENCES:
patent: 4829028 (1989-05-01), Seki et al.
patent: 5711492 (1998-01-01), Cheladze
Patent Abstracts of Japan, vol. 013, No. 262, Jun. 16, 1989 & JP 01 065067 (Iwao Jiki Kogyo KK.).
Patent Abstracts of Japan, vol. 096, No. 002, Feb. 29, 1996 & JP 07 286166 A (Showa Denko KK.).
Database WPI, week 8314, Derwent Publications Ltd., London, GB; & JP 58 032 066 (NGK Spark Plug Co., Ltd.), Feb. 24, 1983.
Imai Yoshihiko
Iwai Akihito
Matsumoto Katsumi
Naito Sosuke
Nakamura Hideki
Hitachi Chemical Co. Ltd.
Kansai Matec Co., Ltd.
Rosenbaum Mark
LandOfFree
Alumina-zirconia sintered body, production thereof, and impact g does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Alumina-zirconia sintered body, production thereof, and impact g, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Alumina-zirconia sintered body, production thereof, and impact g will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1501013