Alloys according to the present invention exhibit good resistance to erosion and stress corrosion cracking. The contents of individual components in these alloys as expressed in terms of wt. % are as follows:
Uehara Toshihiro
Watanabe Rikizo
Agency of Industrial Science and Technology
Yee Deborah
LandOfFree
Alloys having excellent erosion resistance and stress corrosion does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Alloys having excellent erosion resistance and stress corrosion , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Alloys having excellent erosion resistance and stress corrosion will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1474242