ABSTRACT:
A series of braze materials for brazing superalloy substrates at effective brazing temperatures above about 2300.degree. F. is described. The braze materials are formulated as mixtures of cobalt- and nickel-base alloy powders. Each such braze material contains at least two components, one of which is predominantly liquid at the effective brazing temperature, and one of which remains substantially solid at that temperature. The brazing materials solidify by an isothermal solidification process. Unless otherwise limited by the temperature capability of the superalloy substrate being joined, these brazing alloys provide joints that have useful strength at temperatures significantly higher than joints made with prior art brazing alloys.

REFERENCES:
patent: 3482967 (1969-12-01), Redden
patent: 3542543 (1970-11-01), Yount et al.
patent: 3678570 (1972-07-01), Paulonis et al.
patent: 4008844 (1977-02-01), Duvall et al.
patent: 4073639 (1978-02-01), Duvall et al.
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4381944 (1983-05-01), Smith, Jr. et al.
patent: 4389251 (1983-06-01), Simm et al.
patent: 4478638 (1984-10-01), Smith, Jr. et al.
patent: 4705203 (1987-11-01), McComas et al.
patent: 4830934 (1989-05-01), Ferrigno et al.
patent: 4910098 (1990-03-01), Lee et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Alloy powder mixture for brazing of superalloy articles does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Alloy powder mixture for brazing of superalloy articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Alloy powder mixture for brazing of superalloy articles will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2294887

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.