ABSTRACT:
An improved thermal barrier coating system is described. A key feature of the invention is the presence of a thin, adherent aluminum oxide scale on the surface of the substrate. An oxide stabilized ceramic coating is present on the surface of the scale. Preferably, the ceramic coating has a columnar grain structure.
REFERENCES:
patent: Re31339 (1983-08-01), Dardi et al.
patent: 3890956 (1975-06-01), Dils
patent: 4029477 (1977-06-01), Grisik
patent: 4346137 (1982-08-01), Hecht
patent: 4530727 (1985-07-01), Thompson et al.
patent: 4743514 (1988-05-01), Strangman et al.
Fairbanks et al., "High-Rate Sputter Deposition of Protective Coatings on Marine Gas Turbine Hot-Section Superalloys," Jul., 1974, pp. 429-455.
D. Boone et al.: "Advanced Gas Turbine Coatings For Minimally Processed Coal Derived Liquid Fuels"; Fairbanks et al., editors: Dec. 1979.
R. E. Demaray, J. W. Fairbanks and D. H. Boone: "Physical Vapor Deposition of Ceramic Coatings for Gas Turbine Engine Components"; ASME 1982.
T. E. Strangman: "Thermal Barrier Coatings for Turbine Airfoils" Apr. 1984.
Battelle--Final Report Jan. 1985 "Combustion Zone Durability Program".
S. Shen: Technical Progress Report "Development of Improved Corrosion and Erosion Resistance Coatings for Gas Turbine Airfoils"--Reporting period: Oct. 1, 1979 to Apr. 30, 1980.
S. Shen: Final Progress Report "Development of Improved Corrosion and Erosion Resistance Coatings for Gas Turbine Airfoils"--Reporting period: Sep. 1, 1978 to Sep. 30, 1979.
E. Demaray: "Dedicated Electron Beam Reactive Physical Vapor Deposition (R.P.V.D.) Apparatus For The Production Of Ceramic Thermal Barrier Coatings" Project Final Report Dec. 1981.
Demaray et al., "Development of Electron Beam Physical Vapor Deposition of Ceramic Coatings"; Fairbanks et al. editors; May 1982.
Anderson Neal P.
Ulion Nicholas E.
Jenkins Daniel
Rashid James M.
United Technologies Corporation
Walsh Donald P.
LandOfFree
Advanced thermal barrier coated superalloy components does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Advanced thermal barrier coated superalloy components, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Advanced thermal barrier coated superalloy components will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-21296