ABSTRACT:
An adhesive tape which is to be arranged between a lens and at least one of a plurality of chucks in an edge-machining apparatus comprises an adhesive face for being in contact with the lens. A measurement of an adhesive strength of the adhesive face is 4 gf (0.0392 N) or more when a polyethylene terephthalate plate which has been subjected to a surface treatment with a fluorine-modified silicone parting agent is used as a test plate in an adhesive strength test method based on a 180°-peeling method as defined in JIS Z 0237 “adhesive tape/adhesive sheet test method”. A technique which can be used to edge the lens in which an antifouling layer is formed by using a fluorine-containing silane compound having an excellent antifouling effect is also provided.
REFERENCES:
patent: 3631637 (1972-01-01), Tagnon
patent: 5165202 (1992-11-01), Spindel, Jr.
patent: 5341604 (1994-08-01), Wood
patent: 5429838 (1995-07-01), Mansson et al.
patent: 5883169 (1999-03-01), Spector et al.
patent: 5928718 (1999-07-01), Dillon
patent: 6074290 (2000-06-01), Ko et al.
patent: 2002/0149862 (2002-10-01), Wallendorf et al.
patent: 4300673 (1994-07-01), None
patent: 05-078627 (1993-03-01), None
patent: 6-24852 (1994-04-01), None
patent: 4-60923 (1994-05-01), None
patent: 08-229794 (1996-09-01), None
patent: 8-229794 (1996-09-01), None
patent: 09-258003 (1997-10-01), None
patent: 09258003 (1997-10-01), None
patent: 2000-24936 (2000-01-01), None
patent: 2000-024936 (2000-01-01), None
patent: 2000-309759 (2000-11-01), None
patent: 2001-011396 (2001-01-01), None
patent: 2001-64608 (2001-03-01), None
patent: 3275147 (2002-02-01), None
patent: 2002-263998 (2002-09-01), None
patent: 2003-171625 (2003-06-01), None
patent: 2003-311595 (2003-11-01), None
patent: 2004-122238 (2004-04-01), None
patent: 2004-347660 (2004-09-01), None
patent: WO 03/092957 (2003-11-01), None
Search Report from the Singaporean Patent Office dated Nov. 11, 2005.
Computer-generated English Translation of JP 2003-311595.
Computer-generated English Translation of JP 2003-171625.
Computer-generated English Translation of JP 2001-64608.
An Office Action issued in a related foreign application dated Aug. 15, 2006.
Computer generated English Translation of JP 2001-011396.
Computer generated English Translation of JP 2000-309759.
Computer generated English Translation of JP 05-078627.
Computer generated English Translation of JP 3275147.
Katagiri Hiroshi
Kawase Akiko
Suzuki Keiichi
Takeshita Katsuyoshi
Hail III Joseph J.
Muller Bryan R.
Sughrue & Mion, PLLC
LandOfFree
Adhesive tape and edging method using same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Adhesive tape and edging method using same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Adhesive tape and edging method using same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3831842