Additive enhanced solvent deasphalting process (law759)

Mineral oils: processes and products – Refining – Metal contaminant removal

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C208S252000, C208S290000, C208S291000, C208S309000

Reexamination Certificate

active

06245222

ABSTRACT:

FIELD OF THE INVENTION
The present invention relates to the solvent deasphalting of petroleum residuum.
BACKGROUND OF THE INVENTION
Solvent deasphalting is a current process for demetallation of petroleum residuum. The metals concentrate in the solvent-insoluble phase and the deasphalted oil is decreased in metals content. A limitation of art-processes is that as the yield of deasphalted oil increases, so does the metals content. There is a continuing need for refinement of the solvent deasphalting process which produces a high yield of deasphalted oil with a low metals content.
Solvent deasphalting (i.e., extraction of asphaltenes from petroleum stocks is typically accompanied with removal of organometallic, e.g., organo-nickel and vanadium and heteroatoms) is a key aspect of resid upgrading. Solvent deasphalting to produce the foregoing deasphalted oils (DAO) typically is accomplished using suitable hydrocarbonaceous solvents, in particular, hydrocarbons of straight chain paraffins and isoparaffins, containing from 3 to 7 carbon atoms. Most widely known processes are those known as Propane Deasphalting (PDA), Solvent Deasphalting (SDA) and Residual Oil Solvent Deasphalting (ROSE). Solvent deasphalting in this manner is well known in the art, see e.g., U.S. Pat. Nos. 3,975,396; 5,008,838; 5,466,365 and 4,125,458. Applicants' process addresses the “high yield/high metals” limitation of the art.
SUMMARY OF THE INVENTION
The present invention provides for a method for demetallating a metals containing residium by first treating the resid with an additive containing a polyoxy alkylene moiety, preferably an alkyl (polyoxyalkylene) moiety and then treating the resid with a hydrocarbonaceous deasphalting solvent and separating the insoluble phase from the soluble phase containing a deasphalted oil (DAO) having a decreased metals content.
The present invention may comprise, consist or consist essentially of the recited steps or elements and may be practiced in the absence of a step or element not disclosed as required.
DETAILED DESCRIPTION OF THE INVENTION
The present invention provides for a process for enhancing the metals removal capability of solvent deasphalfing processes. Solvent deasphalting is a known process for treatment of petroleum residuua (resid) in which resids are treated with a deasphalting solvent, as known in the art, e.g., alkane solvents such as butane, pentane or heptane. Included in the foregoing are isomers, if any, of the alkanes and alcohols. The process partially decreases the metals content of the deasphalted oil. The process also produces a solvent-insoluble phase (rock) in which the metals removed from the DAO are concentrated. Thus, undesirably as the yield of DAO increases so does the concentration of metals in the DAO.
Applicants have discovered that this limitation of art recognized solvent deasphalting processes can be addressed by the addition of a specific class of additives, i.e., alkane-insoluble polyoxyalkylene group-containing additives prior to addition of the deasphalting solvent. The additive chosen is one that is preferentially insoluble in the deasphalting solvent and preferentially complexes with the organometalic species present in petroleum streams, e.g., species such as organo-nickel, vanadium and iron. Preferential insolubility of the additive in the deasphalting solvent after chelating (complexing) with these metals species is also desired, and thus the deasphalting solvents are chosen such that the resulting additive complex will form a separate phase from the DAO concentrate in the solvent insoluble rock phase.
As stated previously, deasphalting solvents are suitably those known in the art preferably alkanes and related alcohols, e.g., C
2
-C
7
alkanes, C
1
-C
7
alcohols and mixture of said alkanes and alcohols and supercritical CO
2
.
The additive can be added in a small amount of delivery solvent but preferably it is added as is to metals containing petroleum feed and the mixture heated with mixing to achieve sufficient contacting. Upon contacting of the additive-residuum mixture with deasphalting solvent, the resulting additive-metal complex preferentially concentrates in the solvent insoluble rock phase.
Additives suitable for use in the present invention and containing the required polyoxyalkylene group and are represented by compounds of the formula
R—(R
1
O)
m
—H
wherein R is OH or C
8
to C
20
alkyl group which may be unsubstituted or substituted with substantially non-reactive or interfering groups, R
1
is selected from
wherein when R
1
is an ethylene, propylene or butylene oxide moiety, and m is 5-50; and block copolymers of ethylene oxide, propylene oxide and butylene oxide monomers and mixtures thereof having 5000 to 7000 monomer units; and ethylene oxide, propylene oxide and butylene oxide derivatized ethylene diamine. These additives may be obtained from commercial sources or synthesized using known procedures. Examples of suitable additives include: ethylene oxide-polyethylene oxide-ethylene oxide block copolymers (e.g., Pluronics™ family of additives), ethylene oxide-polyethylene oxide derivatized ethylenediamine (e.g., Tectronics™ family of additives) available from BASF.
The additive is present in an effective demetallating amount, typically 0.5 to 20 wt %, preferably 0.5 to 2 wt % based on the weight of the residuum feed.
The additive is contacted with the residuum at temperatures effective to demetallate the resid to produce a treated resid having a decreased metals content. Contacting is carried out at elevated temperature necessary to liquefy or soften the metals containing residuum under pressure. Typically, treatment is at temperatures from about 80-100° C. Pressures sufficient to maintain the deasphalting solvent below its boiling point are suitable.
Deasphalting of the residuum is accomplished by contacting the additive treated residuum with a suitable amount of alkane deasphalting solvent. These are known in the art and include propane, butane, pentane and hexane. The solvents and treatment conditions are known to those skilled in the art. Typical conditions include a ratio of feed to deasphalting solvent from 1:4 to 1:14. However, solvent ratios, temperatures and pressures for deasphalting are known to those skilled in the art.
The treatment results in a DAO and a solvent insoluble material (rock). The DAO has a decreased metals content in comparison to DAO produced by solvent deasphalting without use of the additive.
Included in the types of residuua that may be treated are those having an initial boiling point of 650-1100° F. (343° C. to 593° C.), atmospheric residuum (“AR”) and vacuum residuum (“VR”). However, processed feeds as known to those skilled in the art that contain undesirable metals levels which feeds will be subject to further solvent extraction processes (e.g., DAO) also may be treated. Crude oils and crude oil distillates also may be treated.


REFERENCES:
patent: 2793167 (1957-05-01), Webber
patent: 3975396 (1976-08-01), Bushnell et al.
patent: 4125458 (1978-11-01), Bushnell et al.
patent: 4432865 (1984-02-01), Norman
patent: 5000838 (1991-03-01), Bartilucci et al.
patent: 5466365 (1995-11-01), Savastano et al.
patent: 2579218 (1985-09-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Additive enhanced solvent deasphalting process (law759) does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Additive enhanced solvent deasphalting process (law759), we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Additive enhanced solvent deasphalting process (law759) will most certainly appreciate the feedback.